Hi all.... I recently built my first ebike. 3000w stealth bomber clone. I was to installing the key switch and forgot to unplug the battery before starting. I had it working but I had some wires tangled up and decided to disconnect the the ground connecting to the controller and accidentally touched the ground to the hot wire(rookie move). I got a quick spark and now I can't get it to power on. Did I fry my controller? something else?
Last edited by Bobby Breathes on Jan 30 2020 2:14am, edited 1 time in total.

User avatar
amberwolf   100 GW

100 GW
Posts: 29844
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Did I fry my controller?

Post by amberwolf » Jan 30 2020 12:36am

if the ground and hot wire are the ones to the battery, then it's probably blown it's internal fuse, if it has one. if it doesn't, it may have blown it's bms fets. you'd have to open it up to check, if there's no voltage on it's output.

if the ground and hot wire are the ones to the ocntroller, and the battery was not connected at all when this happened, then there should be nothing wrong, unless there is a fuse in either hot or ground wire to the controller, which could be blown.

you'll have to give specific details and wiring along with what actually touched what, for more specific answers than those guesses.

markz   100 GW

100 GW
Posts: 9414
Joined: Jan 09 2014 11:38pm
Location: Alberta Canada

Re: Did I fry my controller?

Post by markz » Jan 30 2020 1:08am

If your lucky, its a fuse.
If your not so lucky, its a fet.
If your not lucky, its time to fish. How much was the controller you bought? How much is your time worth to you? How much is it to buy a new controller? Maybe buy a cheap controller? Since I got the website open from another post, https://evfittinggreentime.aliexpress.c ... 18ccGmBily

Bobby Breathes   1 µW

1 µW
Posts: 2
Joined: Jan 29 2020 10:46pm

Re: Did I fry my controller? Edit-FIXED

Post by Bobby Breathes » Jan 30 2020 2:16am

I think I just had some faulty wire... I rewired a questionable connection and it working again. Thanks for the help!

markz   100 GW

100 GW
Posts: 9414
Joined: Jan 09 2014 11:38pm
Location: Alberta Canada

Re: Did I fry my controller? Edit-FIXED

Post by markz » Jan 30 2020 11:34pm

Bobby Breathes wrote:
Jan 30 2020 2:16am
I think I just had some faulty wire... I rewired a questionable connection and it working again. Thanks for the help!
Jeeesh I hate when that happens.