Ezee battery fire & recall

Batteries, Chargers, and Battery Management Systems.
Post Reply
Hillhater   100 GW

100 GW
Posts: 10981
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Ezee battery fire & recall

Post by Hillhater » Apr 28 2019 5:20am

Recent house destroying Ebike battery fire in Sydney and a recall on defective Ezee batteries
https://www.smh.com.au/business/consume ... .html?btis
Apparently Ezee are blaming the LG cells for a defect ?
This forum owes its existence to Justin of ebikes.ca

district9prawn   100 W

100 W
Posts: 295
Joined: Jul 20 2013 10:46pm
Location: Sydney

Re: Ezee battery fire & recall

Post by district9prawn » Apr 30 2019 3:46am

Hillhater wrote:
Apr 28 2019 5:20am
Apparently Ezee are blaming the LG cells for a defect ?
And looks like LG deny everything. I don't recall reading that in article on the day it was published. I only noticed it today?
Neu 8057 6kW left hand drive hardtail with 18 fet Vesc: viewtopic.php?f=6&t=96754

User avatar
Matador   10 kW

10 kW
Posts: 941
Joined: Jun 29 2016 10:00pm

Re: Ezee battery fire & recall

Post by Matador » May 28 2019 4:56pm

Faulty BMS also likely ... To allow overcharging a cell group to a point of unstability. I'm thinking, at leas 4.4V...

billvon   1 GW

1 GW
Posts: 3051
Joined: Sep 16 2007 9:53pm
Location: san diego

Re: Ezee battery fire & recall

Post by billvon » May 28 2019 4:58pm

Matador wrote:
May 28 2019 4:56pm
Faulty BMS also likely ... To allow overcharging a cell group to a point of unstability. I'm thinking, at leas 4.4V...
Or a puncture. Or an internal short. A little early to be deciding it's overcharge.
--bill von

Hillhater   100 GW

100 GW
Posts: 10981
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Ezee battery fire & recall

Post by Hillhater » May 28 2019 6:23pm

I assume Ezee did do some basic inspection and checks to eliminate obvious faults before they issued a recall , let alone finger a reputable cell manufacturer like LG.
This forum owes its existence to Justin of ebikes.ca

User avatar
Matador   10 kW

10 kW
Posts: 941
Joined: Jun 29 2016 10:00pm

Re: Ezee battery fire & recall

Post by Matador » May 28 2019 8:41pm

billvon wrote:
May 28 2019 4:58pm
Matador wrote:
May 28 2019 4:56pm
Faulty BMS also likely ... To allow overcharging a cell group to a point of unstability. I'm thinking, at leas 4.4V...
Or a puncture. Or an internal short. A little early to be deciding it's overcharge.
Internal short also good possibility. But puncture ? The battery was left charging ovenight, left unattended. So puncture not impossible but seems unlikely.

Maador

User avatar
neptronix   100 GW

100 GW
Posts: 14247
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: Ezee battery fire & recall

Post by neptronix » May 28 2019 9:20pm

I love how she just put a new battery on the bike and kept riding...

Thug life! 8)
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

Post Reply