ecotech   100 mW

100 mW
Posts: 43
Joined: Nov 12 2016 4:56pm

Re: Thread for new battery breakthrough PR releases

Post by ecotech » Jan 10 2017 10:55am

icherouveim wrote:The secret is the graphene. They say it is going to change the future.
I am very happy with my new 10AH graphene cells from WESTART factory, I can charge them in mimutes with 30A without any problems.
in the future they are going to be much more powerful when the companies will be able to take the full advantage of the graphene.

Nop graphene isn't the answer, even if they say graphene on the outside I doubt it's really used, big battery manufacturers use regular graphite for their cells, graphene is over-hyped carbon.

User avatar
Arlo1   100 GW

100 GW
Posts: 8376
Joined: Apr 26 2009 10:36pm
Location: Nanaimo
Contact:

Re: Thread for new battery breakthrough PR releases

Post by Arlo1 » Jan 10 2017 11:18am

ecotech wrote:
icherouveim wrote:The secret is the graphene. They say it is going to change the future.
I am very happy with my new 10AH graphene cells from WESTART factory, I can charge them in mimutes with 30A without any problems.
in the future they are going to be much more powerful when the companies will be able to take the full advantage of the graphene.

Nop graphene isn't the answer, even if they say graphene on the outside I doubt it's really used, big battery manufacturers use regular graphite for their cells, graphene is over-hyped carbon.

LMFAO. I have some graphite here and it doesn't even conduct as well as copper. Graphene is used the a lot of GOOD cells incl. Zero motorcycles.
Last edited by Arlo1 on Jan 10 2017 5:59pm, edited 2 times in total.
Does your project need a high performance motor drive, battery charger or other power electronics developed? Let's talk!
www.powerdesigns.ca
Leaf motor controller build. http://endless-sphere.com/forums/viewto ... 27#p963227
YSR build http://www.youtube.com/watch?v=BRo8r5g4NBg
Never above 4.2v never below 2.7v EVER!!!
Support me on Patreon. https://www.patreon.com/user/posts?u=6842045
http://www.undergroundelectrics.ca/

User avatar
zzoing   10 kW

10 kW
Posts: 732
Joined: Feb 01 2008 12:26am
Location: Fr SE

Re: Thread for new battery breakthrough PR releases

Post by zzoing » Jan 10 2017 2:27pm

Overhyped graphene: www.youtube.com/watch?v=R5dwdZCKBZM
[youtube]https://youtu.be/R5dwdZCKBZM[/youtube]
https://www.engadget.com/2017/01/09/mit ... han-steel/

we may even have entire bikes made out of graphene composites one day.

graphene news is quite good:

https://www.google.fr/search?q=graphene ... 94&bih=567

User avatar
liveforphysics   100 GW

100 GW
Posts: 14134
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: Thread for new battery breakthrough PR releases

Post by liveforphysics » Jan 10 2017 4:28pm

Graphene is a remarkable material in so many ways.

Something odd though, in an anode it improves performance only up to something like 0.3% of the anode being graphene with the remainder being graphite and binders. If you increase the amount of graphene beyond that it decreases cell performance (at least in the test data I've seen).

Graphene has been used almost universally in EV cells for at least the last 4 years, but wasn't commonly talked about until it became more of a marketing hype term.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

User avatar
Wheazel   10 kW

10 kW
Posts: 969
Joined: Nov 02 2010 2:30pm
Location: Sundsvall, Sweden

Re: Thread for new battery breakthrough PR releases

Post by Wheazel » Jan 28 2017 8:19am

liveforphysics wrote:Graphene is a remarkable material in so many ways.

Something odd though, in an anode it improves performance only up to something like 0.3% of the anode being graphene with the remainder being graphite and binders. If you increase the amount of graphene beyond that it decreases cell performance (at least in the test data I've seen).

Graphene has been used almost universally in EV cells for at least the last 4 years, but wasn't commonly talked about until it became more of a marketing hype term.
Do you know the reason for the diminishing gains in the anode?

User avatar
liveforphysics   100 GW

100 GW
Posts: 14134
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: Thread for new battery breakthrough PR releases

Post by liveforphysics » Jan 28 2017 4:14pm

Wheazel wrote:
liveforphysics wrote:Graphene is a remarkable material in so many ways.

Something odd though, in an anode it improves performance only up to something like 0.3% of the anode being graphene with the remainder being graphite and binders. If you increase the amount of graphene beyond that it decreases cell performance (at least in the test data I've seen).

Graphene has been used almost universally in EV cells for at least the last 4 years, but wasn't commonly talked about until it became more of a marketing hype term.
Do you know the reason for the diminishing gains in the anode?

Nope! But it's a similar trend with adding SWCNTs (single wall carbon nanotubes), they help in a tiny amount and hurt in a greater amount. I couldn't begin to explain why.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

User avatar
LockH   100 GW

100 GW
Posts: 17582
Joined: Jul 09 2013 11:06pm
Location: Ummm.. Started out in Victoria BC Canada, then started to move around... Oh oh.

Re: Thread for new battery breakthrough PR releases

Post by LockH » Feb 01 2017 7:17am

Company "Ionic Materials, Inc.":
http://ionicmaterials.com/

(They say:)
Ionic Materials is a technology company focused on developing materials for batteries. At the core of our value proposition is a new solid polymer that has all of the properties required to replace the liquid electrolytes used in currently-available batteries.
Image

... and:
Ionic Materials’ polymer is a true platform technology that enables a wide range of next generation battery chemistries including lithium metal anodes, high voltage intercalation cathodes, sulfur conversion cathodes and a proprietary system that we refer to as our “High Wh/L” chemistry. All of these chemistries have potential to dramatically improve performance and safety, and reduce costs compared to conventional lithium ion systems.
Spotted as being intro'ed on upcoming PBS series:
http://finance.yahoo.com/news/exclusive ... 45984.html
ES changed my life (for the waaaaay better).

Eff. June, 2014 Phoenix Ebike Promotions

(Current ride? High speed lawn chair.)
viewtopic.php?f=3&t=57408

Phoenix Ebike Promotions conversion kit (work in progress. More drink holders, etc etc)
viewtopic.php?f=15&t=60564

Joined yer local chapter of EA yet?
(Ebikers Anonymous - Where we're all miserable failures, but the parties are hilarious...)

hypertoric_amplituhedron   100 W

100 W
Posts: 216
Joined: Dec 02 2016 7:57pm
Location: Land of the Florida Man

Re: Thread for new battery breakthrough PR releases

Post by hypertoric_amplituhedron » Feb 02 2017 9:18pm

Wow, this is awesome. The days of a 10kwh triangle pack are coming. Might want to invest some stock, or wait for the next supercapacitor.
There are two types of people in this world.

1. Those who can extrapolate from missing information.

User avatar
Arlo1   100 GW

100 GW
Posts: 8376
Joined: Apr 26 2009 10:36pm
Location: Nanaimo
Contact:

Re: Thread for new battery breakthrough PR releases

Post by Arlo1 » Feb 03 2017 2:17am

Does your project need a high performance motor drive, battery charger or other power electronics developed? Let's talk!
www.powerdesigns.ca
Leaf motor controller build. http://endless-sphere.com/forums/viewto ... 27#p963227
YSR build http://www.youtube.com/watch?v=BRo8r5g4NBg
Never above 4.2v never below 2.7v EVER!!!
Support me on Patreon. https://www.patreon.com/user/posts?u=6842045
http://www.undergroundelectrics.ca/

DVDRW   100 W

100 W
Posts: 211
Joined: Sep 10 2012 10:57am
Location: Tallinn, Estonia, EU
Contact:

Re: Thread for new battery breakthrough PR releases

Post by DVDRW » Feb 03 2017 11:55pm

New cell, price breakthrough? Sanyo UR18650AAN
1,59€

User avatar
Matador   10 kW

10 kW
Posts: 915
Joined: Jun 29 2016 10:00pm

Re: Thread for new battery breakthrough PR releases

Post by Matador » Feb 05 2017 12:48pm

New Tesla Cells :

Clearly the journalist doesn't know his facts very well, especially not how to calculate the volume of a cell cylinder...

In truth the figures looks more like that IMHO :

Going from 18650 (18 x 65.0 mm) : around 3450 mAh for 16.540 mL volume (aka 16.54 cc) and 50g at 3.6V nominal.
To 21700 (21 x 70.0 mm) : around 4750 mAh for 24.245 mL volume and 75 g at 3.6V nominal.

Image
REF for this picture : http://www.candlepowerforums.com/vb/sho ... -Elon-Musk
Uploaded here for archive pruposes... if URL for picture is ever deleted
9iobu.jpg
9iobu.jpg (71.93 KiB) Viewed 1641 times

That's going from 208.6 mAh/mL to 186.0 mAh/mL @ 3.6 nominal volts : that's going from 751 to 670 Wh/L. So a slight decrease in Volumetric Energy Density.
That's going from 69.0 mAh/g to 63.3 mAh/g @ 3.6 nominal volts : that's going from 248.4 Wh/kg to 228.0 Wh/kg. So a slight decrease in Massic Energy Density.
So Telsa is choosing cells that have 10.8 % less energy density per volume units and 8.2% less energy density per mass units...

Why is Telsa doing this change if the cells packs less energy per volume and less energy per mass ?

crazymanc   100 mW

100 mW
Posts: 37
Joined: Sep 04 2016 8:55pm

Re: Thread for new battery breakthrough PR releases

Post by crazymanc » Feb 05 2017 2:39pm

It isn't just about energy density but about current delivery and discharge characteristics.

A lot of the 3400+ mAh batteries can only provide this capacity at 0.1C. And when compared at higher rates of discharge, you can often find that the 'high discharge optimised' ~2900mAh 18650s outperform, or are equivalent in apparent capacity, to their higher 'paper rating' capacity brothers.

Tesla will have designed their batteries for high current delivery and longevity under such circumstances, no doubt sacrificing some absolute capacity in doing so.

This new polymer electrolyte seems very appealing though.

hypertoric_amplituhedron   100 W

100 W
Posts: 216
Joined: Dec 02 2016 7:57pm
Location: Land of the Florida Man

Re: Thread for new battery breakthrough PR releases

Post by hypertoric_amplituhedron » Feb 05 2017 3:36pm

This new polymer electrolyte seems very appealing though.
Yes it does. They've already doubled the capacity with the first prototype. Going out on a stretch, but improving their design could, for all we know, lead to triple or quadruple the capacity. Or, imagine building a custom solid state battery with a 3D printer. One solid chunk shaped however you like.
There are two types of people in this world.

1. Those who can extrapolate from missing information.

crazymanc   100 mW

100 mW
Posts: 37
Joined: Sep 04 2016 8:55pm

Re: Thread for new battery breakthrough PR releases

Post by crazymanc » Feb 05 2017 8:08pm

Well I'd imagine that a heavily optimised polymer electrolyte battery would require a bit more than a 3D printer to get the most out of it, but that does present an interesting thought. Currently the liquid electrolyte is nasty stuff and presumably requires somewhat expensive production methods. Both in terms of safety and the actual machinery on the production line. Working with liquids isn't nice.

At the very least a polymer electrolyte should be far easier (and less costly) to deal with, both in terms of building the batteries and in safely shipping them, once made. I mean I know we talk about energy density being the most important factor, but cost is too.

If the batteries were inherently safe and cheap we could actually end up with a situation where we could potentially overcharge them, for greater capacity, then once the batteries are at reduced point in their life cycle, trade them out for something new and relegate the older batteries to grid storage.

Well that's just a thought.

If the batteries do genuinely have at least double the capacity, I can't see there being much need for that.

As to whether this change could yield batteries with 4x the capacity to what we see now... That's entirely possible. Although basic lithium tech is well understood, this polymer is in its infancy, as are the other benefits it allows, such as using lithium metal within the battery itself.

At the moment the polymer electrolyte is at the proof of concept stage. Once it's been successfully proven, big r&d departments can get their hands on it and really get to work on optimising it.

User avatar
macribs   1.21 GW

1.21 GW
Posts: 3654
Joined: Jul 22 2014 5:59pm

Re: Thread for new battery breakthrough PR releases

Post by macribs » Feb 05 2017 8:50pm

One happy side effect of that new polymer battery would be the freedom to ship batteries any way the buyer prefers. By air, sea or land.
Now more insane safety regulations regarding shipping for the fail safe polymer battery. The added capacity or discharge rate will be a nice bonus on top.

User avatar
liveforphysics   100 GW

100 GW
Posts: 14134
Joined: Oct 29 2008 1:48am
Location: Santa Cruz, CA, USA

Re: Thread for new battery breakthrough PR releases

Post by liveforphysics » Feb 05 2017 10:10pm

The demonstrated (lab prototypes) high cycle life and safe cell energy density record is something like 1150Wh/kg IIRC.

The physics permit >5,000Wh/kg if you had the right materials tech.

Supercaps that were built as atom scale perfect graphene plate supercaps can also be multiple kWh/kg, but it's not yet known how to make that level of precision structure.

Electrical energy storage is limited almost directly by a combination of material technology and manufacturing technology that scales efficiently.
Each carcinogen vapor exposure includes a dice roll for cancer.

Each mutagen vapor exposure includes a dice roll for reproductive genetic defects in your children.

Each engine start sprays them into a shared atmosphere which includes beings not offered an opportunity to consent accepting these cancer experiences and defective genetics life experiences.

Every post is a free gift to the collective of minds composing the living bleeding edge of LEV development on our spaceship.

Hanssing   100 mW

100 mW
Posts: 46
Joined: Aug 06 2016 6:57am

Re: Thread for new battery breakthrough PR releases

Post by Hanssing » Feb 11 2017 5:29am

http://www.renewableenergyworld.com/art ... SS+Feed%29

http://www.pnas.org/content/114/5/834.full (Paywalled)

https://en.wikipedia.org/wiki/Urea
“So essentially, what you have is a battery made with some of the cheapest and most abundant materials you can find on Earth. And it actually has good performance,” said Dai. “Who would have thought you could take graphite, aluminum, urea, and actually make a battery that can cycle for a pretty long time?”

All the way back from 17th. January, using Aluminum + urea (ie. mammal urin).
Tech is for gridstorage.

User avatar
LockH   100 GW

100 GW
Posts: 17582
Joined: Jul 09 2013 11:06pm
Location: Ummm.. Started out in Victoria BC Canada, then started to move around... Oh oh.

Re: Thread for new battery breakthrough PR releases

Post by LockH » Feb 11 2017 9:35pm

Silicon will blow lithium batteries out of water, says Adelaide firm:
http://www.afr.com/news/silicon-will-bl ... 207-gu7eg7

Starts:
An Adelaide company has developed a silicon storage device that it claims costs a tenth as much as a lithium ion battery to store the same energy and is eyeing a $10 million public float.

1414 Degrees had its origins in patented CSIRO research and has built a prototype molten silicon storage device which it is testing at its Tonsley Innovation Precinct site south of Adelaide.

Chairman Kevin Moriarty says 1414 Degrees' process can store 500 kilowatt hours of energy in a 70-centimetre cube of molten silicon – about 36 times as much energy as Tesla's 14KWh Powerwall 2 lithium ion home storage battery in about the same space.

Put another way, he says the company can build a 10MWh storage device for about $700,000. The 714 Tesla Powerwall 2s that would be needed to store the same amount of energy would cost $7 million before volume discounts.
ES changed my life (for the waaaaay better).

Eff. June, 2014 Phoenix Ebike Promotions

(Current ride? High speed lawn chair.)
viewtopic.php?f=3&t=57408

Phoenix Ebike Promotions conversion kit (work in progress. More drink holders, etc etc)
viewtopic.php?f=15&t=60564

Joined yer local chapter of EA yet?
(Ebikers Anonymous - Where we're all miserable failures, but the parties are hilarious...)

User avatar
Arlo1   100 GW

100 GW
Posts: 8376
Joined: Apr 26 2009 10:36pm
Location: Nanaimo
Contact:

Re: Thread for new battery breakthrough PR releases

Post by Arlo1 » Feb 11 2017 11:16pm

Does that mean it needs to be kept at 1414 deg? How much energy does that take?
Does your project need a high performance motor drive, battery charger or other power electronics developed? Let's talk!
www.powerdesigns.ca
Leaf motor controller build. http://endless-sphere.com/forums/viewto ... 27#p963227
YSR build http://www.youtube.com/watch?v=BRo8r5g4NBg
Never above 4.2v never below 2.7v EVER!!!
Support me on Patreon. https://www.patreon.com/user/posts?u=6842045
http://www.undergroundelectrics.ca/

User avatar
amberwolf   100 GW

100 GW
Posts: 30442
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Thread for new battery breakthrough PR releases

Post by amberwolf » Feb 12 2017 1:07am

To reach that temperature, or to keep it there?

To reach it is probably something similar to it's storage capacity plus conversion inefficiencies/insulation losses.

To keep it there would depend on whatever the insulation level is, so the better insulated the less energy needed to keep it there.

User avatar
Arlo1   100 GW

100 GW
Posts: 8376
Joined: Apr 26 2009 10:36pm
Location: Nanaimo
Contact:

Re: Thread for new battery breakthrough PR releases

Post by Arlo1 » Feb 12 2017 1:56am

amberwolf wrote:To reach that temperature, or to keep it there?

To reach it is probably something similar to it's storage capacity plus conversion inefficiencies/insulation losses.

To keep it there would depend on whatever the insulation level is, so the better insulated the less energy needed to keep it there.
Yes was rhetorical its quite the idea and will take some energy (and safety considerations) to make it happen.
Does your project need a high performance motor drive, battery charger or other power electronics developed? Let's talk!
www.powerdesigns.ca
Leaf motor controller build. http://endless-sphere.com/forums/viewto ... 27#p963227
YSR build http://www.youtube.com/watch?v=BRo8r5g4NBg
Never above 4.2v never below 2.7v EVER!!!
Support me on Patreon. https://www.patreon.com/user/posts?u=6842045
http://www.undergroundelectrics.ca/

User avatar
TheBeastie   10 MW

10 MW
Posts: 2020
Joined: Jul 28 2012 12:31am
Location: Melbourne Australia

Re: Thread for new battery breakthrough PR releases

Post by TheBeastie » Feb 12 2017 7:27am

LockH wrote:Silicon will blow lithium batteries out of water, says Adelaide firm:
http://www.afr.com/news/silicon-will-bl ... 207-gu7eg7
Arlo1 wrote:
amberwolf wrote:To reach that temperature, or to keep it there?

To reach it is probably something similar to it's storage capacity plus conversion inefficiencies/insulation losses.

To keep it there would depend on whatever the insulation level is, so the better insulated the less energy needed to keep it there.
Yes was rhetorical its quite the idea and will take some energy (and safety considerations) to make it happen.
Adelaide is a major AU city that tends to get a lot of days over 40degrees celsius during the summer, I think its helped cause them to become quite a pro-renewable energy state which they have been for a while now with up to %45 reliance on renewable energy.

The thing is Adelaide has been a lot in the local AU news lately because of high renewable energy reliance and a fair amount of electricity blackouts as well as having some of the most expensive electricity prices in the world according to Wikipedia, I don't think it's a coincidence that this new energy storage idea came out days after its recent most widely reported blackout in the media.

It's often said that the electricity grid is the most complex piece of infrastructure in the developed world. Adding into the grid renewable energy makes this most complex piece of infrastructure at least twice as complex to manage, this ABC 7:30 report touches on SAs recent blackouts but fails to connect the two issues together but its still worth checking out if you find this stuff interesting.
http://www.abc.net.au/7.30/content/2017/s4617366.htm
http://www.abc.net.au/7.30/content/2017/s4633511.htm
Germany has increased at least 7 times its annual grid management costs over the last few years trying to manage the stability of its grid when merging in new windfarm sources etc.

There is a large coal power plant in Victoria that's getting shut down next month and South Australia/Adelaide buys a lot of power from Victoria, the state grid interconnect is always running at full capacity.
So there is a lot of tension and blame going around, its going to get interesting when the Victorian hazelwood power station does shut down next month.
https://en.wikipedia.org/wiki/Hazelwood_Power_Station
Last edited by TheBeastie on Mar 11 2017 12:13am, edited 4 times in total.
Speed Kills Range, 10mph = 46 miles range, 20mph = 20 miles, 30mph = 8 miles rangehttps://goo.gl/1JNL53
Over Charging Kills ur battery bit.ly/1hzWKl4
Consider PAS as your only throttle https://goo.gl/Kg1F8F
Fuel-Cell is the ultimate battery coupled with 4th-gen Nuclear
https://goo.gl/TcKtHs https://goo.gl/ZhFFot https://goo.gl/gfa215
10 Square Miles of solar panels = 0.12GW average power! https://goo.gl/Ub1S39

User avatar
LockH   100 GW

100 GW
Posts: 17582
Joined: Jul 09 2013 11:06pm
Location: Ummm.. Started out in Victoria BC Canada, then started to move around... Oh oh.

Re: Thread for new battery breakthrough PR releases

Post by LockH » Feb 12 2017 9:50am

^^ Hehe... Their web site:
http://1414degrees.com.au/
ES changed my life (for the waaaaay better).

Eff. June, 2014 Phoenix Ebike Promotions

(Current ride? High speed lawn chair.)
viewtopic.php?f=3&t=57408

Phoenix Ebike Promotions conversion kit (work in progress. More drink holders, etc etc)
viewtopic.php?f=15&t=60564

Joined yer local chapter of EA yet?
(Ebikers Anonymous - Where we're all miserable failures, but the parties are hilarious...)

Hillhater   100 GW

100 GW
Posts: 10914
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Thread for new battery breakthrough PR releases

Post by Hillhater » Feb 12 2017 8:46pm

from their site....
...The prototype had its first run on September 30, producing better than expected results at such an early stage of testing using less than 50% silicon load. Peak electrical output from the Stirling engine and generator was 30.4kW during the first run on stored latent heat recovering 20kWh. The Electrical Recovery Device (ERD) efficiency was 31% while the Combined Heat and Power (CHP) efficiency was better than 80%.......
so, the Electrical efficiency isnt too clever at the moment, but if you need heat as well then it could be useful.
....But i dont think Adelaide needs any more heat currently !
This forum owes its existence to Justin of ebikes.ca

Rube   100 W

100 W
Posts: 254
Joined: Jun 25 2016 10:18pm
Location: Brisbane, Australia

Re: Thread for new battery breakthrough PR releases

Post by Rube » Feb 13 2017 4:28am

My theory is the design complements a heliostat in a solar thermal energy/ desalination plant in Port Augusta AU.
http://reneweconomy.com.au/world-first- ... sta-41643/

In a country/ state with limited high cost arable land, large solar potential and a distributed population; solar thermal energy and low cost batteries complement the transition from coal, and the uptake of existing wind and solar generation.

The big issues is inertia in the grid, non competitive coal power stations are valued because of inertia in the generators. The inertia is a load buffer to keep the supply frequency within range especially when 35 -40C (95-104) days are common in summer.

Hydro is a option for inertia storage, turn the tap to up output but environmental impact and limited water mean high temp batteries may make sense. I'm no expert so interested in the communities' thoughts.

Post Reply