Wanted: One 16s Li-ION BMS

Looking for something? Need a special part, but can't find it online anywhere? Post what you need, maybe others will have it to sell. Guest may post replies to topics already here. All topics here will expire after 60 days of inactivity.
Post Reply
The Mighty Volt   10 MW

10 MW
Posts: 2254
Joined: Oct 17 2009 9:35am
Location: Republic of Ireland.

Wanted: One 16s Li-ION BMS

Post by The Mighty Volt » Aug 11 2019 3:01pm

Hi, I am building a triangle pack for a home made ebike.

I'd prefer one discharge point and one charge point.

50A discharge OR MORE ideally, not too pushed about the charge amps.

Not interested in the usual £14.99 jobs that don't work.

Something with big ugly resistors if necessary, I need this thing to really balance a pack.

This battery is getting built into a triangle frame and left there, I don't want to be taking it out and putting it back.

Thanks.

User avatar
Matador   10 kW

10 kW
Posts: 911
Joined: Jun 29 2016 10:00pm

Re: Wanted: One 16s Li-ION BMS

Post by Matador » Aug 11 2019 8:16pm

Try Bestech power website

User avatar
amberwolf   100 GW

100 GW
Posts: 29844
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Wanted: One 16s Li-ION BMS

Post by amberwolf » Aug 12 2019 12:15am

The Mighty Volt wrote:
Aug 11 2019 3:01pm
Something with big ugly resistors if necessary, I need this thing to really balance a pack.
How damaged are the cells already?

If they're new well-matched cells of good quality, being used well within their limits, you won't have to worry much about balancing, especially if the BMS has a proper (meaning above absolute minimum) cell-level LVC so the pack doesn't get run down to nothing.

If they're worn out used recycled cells of various kinds mixed together...well, then you probably do need a better balancer, if you want it to balance while still quickly charging it.

;)

The Mighty Volt   10 MW

10 MW
Posts: 2254
Joined: Oct 17 2009 9:35am
Location: Republic of Ireland.

Re: Wanted: One 16s Li-ION BMS

Post by The Mighty Volt » Aug 12 2019 1:11pm

Hi Amberwolf.

The pack hasn't even been made, I got 100 cells from a guy online and they are all, so far, 3.869v or so.

They look good.

I basically I just need something that will not allow me to drag the pack down or over charge it.

Thanks.

The Mighty Volt   10 MW

10 MW
Posts: 2254
Joined: Oct 17 2009 9:35am
Location: Republic of Ireland.

Re: Wanted: One 16s Li-ION BMS

Post by The Mighty Volt » Aug 12 2019 1:24pm

Matador wrote:
Aug 11 2019 8:16pm
Try Bestech power website
Cheers! :bigthumb: