Modular Rebuildable Repairable 18650 battery.

Post by shawname » Feb 10 2016 7:53pm

Thought I'd introduce a way of assembling 18650 cells into a battery that does not commit the cells by spot welding. The battery can be disassembled to be repaired, to have the cells upgraded, or reconfigured to change voltage or ampacity.

"BatteryBlocs®" are built from parallel groups of 4, 6, 8 and 10 cells. The cells are held together with "magnetic compression." The Blocs are stacked to multiply voltage and/or amperage. They are designed to fit into 4 inch plastic fencepost sheaths, but can also be assembled into a powerwall or even a radial design. I think they look real cool, and I love showing off my batteries.

I saw the need for a battery I could control after disappointments with Chinese made batteries. I worked for a couple of years designing and testing the concept, and when I thought I couldn't improve it anymore I tested it by riding my Mundo around the USA on a door to door 4 month 9,750 mile journey. Upon returning, I took the lessons learned and refined the battery case design into what it is today, there is a patent pending. The book is on Amazon, "Loop the USA, an ebike Odyssey", by Shawn McCarty.

I'm just starting to market the cases and would appreciate feedback. http://www.batteryblocs.com

Image

[moderator edit to fix link, and add pic]

Hillhater   100 GW

100 GW
Posts: 10978
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Modular Rebuildable Repairable 18650 battery.

Post by Hillhater » Feb 10 2016 10:59pm

Any testing done on the resistance of the magnets compared to spot welded connections ?
This forum owes its existence to Justin of ebikes.ca

Scottydog   100 W

100 W
Posts: 156
Joined: Oct 26 2013 10:45am

Re: Modular Rebuildable Repairable 18650 battery.

Post by Scottydog » Feb 11 2016 9:17am

Personally I'm quite impressed! I think the concept of small mini modules makes it easier to maintain good pressure on the connections with the tensioning bolts. Obviously the bolts needed to be plastic, but is the idea that they create a degree of elasticity and keep even pressure? The modular system is great!

I've often thought about 18650 packs, but purchasing complete welded ones for massive capacities seemed daunting.

Personally I think plated copper plates would be more appealing, the steel ones less so, though I guess a degree of stiffness is important? Aluminium perhaps? Would a conductive paste also be good?

I liked the video explanations, only watched one.

Didn't check you page, but to have the full dimensions for each size along with assembled weights would be good also!

awesome job!

Scottydog   100 W

100 W
Posts: 156
Joined: Oct 26 2013 10:45am

Re: Modular Rebuildable Repairable 18650 battery.

Post by Scottydog » Feb 11 2016 9:19am

Just saw the calculator on the website! Awesome going to download! :D

Scottydog   100 W

100 W
Posts: 156
Joined: Oct 26 2013 10:45am

Re: Modular Rebuildable Repairable 18650 battery.

Post by Scottydog » Feb 11 2016 9:26am

I see the ones on the site look 3D printed, are the production ones to be molded of some sort?

Also the addition of pack size and weight would be good. That addition to the spreadsheets could be good.

shawname   1 W

1 W
Posts: 59
Joined: Apr 01 2011 7:45am
Location: Venice, Florida
Contact:

Re: Modular Rebuildable Repairable 18650 battery.

Post by shawname » Feb 11 2016 11:25am

Hillhater wrote:Any testing done on the resistance of the magnets compared to spot welded connections ?
15 magnets stack to about 1" with no measurable resistance on my ohm meter. They are nickel plated neodymium.

shawname   1 W

1 W
Posts: 59
Joined: Apr 01 2011 7:45am
Location: Venice, Florida
Contact:

Re: Modular Rebuildable Repairable 18650 battery.

Post by shawname » Feb 11 2016 11:36am

Scottydog wrote:Personally I'm quite impressed! I think the concept of small mini modules makes it easier to maintain good pressure on the connections with the tensioning bolts. Obviously the bolts needed to be plastic, but is the idea that they create a degree of elasticity and keep even pressure? The modular system is great!

I've often thought about 18650 packs, but purchasing complete welded ones for massive capacities seemed daunting.

The battery I looped the USA with was a 68 amp hour 50.4 (14S) battery. That's 3.4 KW. Working on a 100 volt 44 amp one for a customer- with a 125 amp draw!


Personally I think plated copper plates would be more appealing, the steel ones less so, though I guess a degree of stiffness is important? Aluminium perhaps? Would a conductive paste also be good?

Sure gave this some thought, and did the math, but the galvanized steel is magnetic, and not much less conductive than nickel. Used in .032 thickness it has very little resistance. The connectors can always be doubled for even less resistance.


I liked the video explanations, only watched one.

Didn't check you page, but to have the full dimensions for each size along with assembled weights would be good also!

Hmmm, yes, they are in the products page. At least the dimensions. I should put the weight as well, thanks.

awesome job!
Thanks!

shawname   1 W

1 W
Posts: 59
Joined: Apr 01 2011 7:45am
Location: Venice, Florida
Contact:

Re: Modular Rebuildable Repairable 18650 battery.

Post by shawname » Feb 11 2016 11:49am

Yes, the plastic parts of the cases are 3d printed from PLA. They are complex and 3d printing is very cost effective. Injection molding would give a better finish, but I can't justify the cost of the molds.

The plastic parts hold up quite well when not exposed to the elements. If left in the sun or exposed on an ebike, they can be brushed with Spar Varnish, which gives a nice shiny protective shell and provides UV protection.

User avatar
Grizzl-E   100 W

100 W
Posts: 206
Joined: Jun 01 2015 9:57pm
Location: Manitoba, Canada

Re: Modular Rebuildable Repairable 18650 battery.

Post by Grizzl-E » Feb 11 2016 12:45pm

Hey if you haven't tried it yet pick up some petg filament. It prints almost as easy as pla but is stronger than abs. It's become my new go to filament for anything production.
Only brutal acceleration will do.

User avatar
bowlofsalad   1 MW

1 MW
Posts: 1540
Joined: Feb 01 2013 10:28pm
Location: Midwest, USA

Re: Modular Rebuildable Repairable 18650 battery.

Post by bowlofsalad » Feb 11 2016 1:57pm

shawname wrote:
Hillhater wrote:Any testing done on the resistance of the magnets compared to spot welded connections ?

The magnets are nickel plated neodymium. A 1" stack - 15 magnets- shows no measurable resistance on my Klein ohmmeter.
Are you using galvanized steel for these kits?

shawname   1 W

1 W
Posts: 59
Joined: Apr 01 2011 7:45am
Location: Venice, Florida
Contact:

Re: Modular Rebuildable Repairable 18650 battery.

Post by shawname » Feb 11 2016 2:41pm

Yes, I am using galvanized 1010 steel. The steel is 12% as conductive as copper. The zinc coating is 27% as conductive as copper.

Compared to spot welding? You need resistance to weld. Solid nickel strips are 22% as conductive as copper. And the battery builder may have used nickel plated steel- it's the most common connector. And the strips are small compared to BatteryBlocs connectors.

The larger the connector the less resistance. And the larger the connection area the less resistance. That's why BatteryBlocs' connectors are massive and the tops are open to allow massive contact area.

I'm not saying one way is better than another, I do both in my shop depending on the job. I spot weld when I have to fit the cells into a small preexisting case. But when I am just building a battery, I go for the modularity and solidness of BatteryBlocs.

Staying with the same material also prevents galvanic action- it plagued me on some of the earlier aluminum/stainless designs!

Scottydog   100 W

100 W
Posts: 156
Joined: Oct 26 2013 10:45am

Re: Modular Rebuildable Repairable 18650 battery.

Post by Scottydog » Feb 11 2016 2:56pm

I watched the videos, see magnets are used also, that makes the need for the steel correct? Neat design, the fence post packaging is a good one! :D

shawname   1 W

1 W
Posts: 59
Joined: Apr 01 2011 7:45am
Location: Venice, Florida
Contact:

Re: Modular Rebuildable Repairable 18650 battery.

Post by shawname » Feb 11 2016 5:56pm

Cool, thanks for taking the time.

Yes, the fence posts work great. They are a good size, 4" fits between the knees!

I'll do another video soon on the endcaps- with cell loggers and xt60 and xt90 connectors and sensor wire connections.

shawname   1 W

1 W
Posts: 59
Joined: Apr 01 2011 7:45am
Location: Venice, Florida
Contact:

Re: Modular Rebuildable Repairable 18650 battery.

Post by shawname » Feb 19 2016 9:45am

I've been working with the PTEG filament on your suggestion, thank you. It does print well. It bridges less well than PLA, and there is a big bridge on the BatteryBloc case. Also, it is less rigid than PLA..... I can see where this would be desirable in some cases, but I like the structural integrity of PLA for BatteryBlocs.

Thanks for the suggestion though.

User avatar
Grizzl-E   100 W

100 W
Posts: 206
Joined: Jun 01 2015 9:57pm
Location: Manitoba, Canada

Re: Modular Rebuildable Repairable 18650 battery.

Post by Grizzl-E » Feb 26 2016 10:14pm

No worries. Glad to see you making this idea work and available. I have been trying a similar base concept with milled pcb boards on either side of a printed spacer pack. Partially to make it rebuildable and partially to make it easier to travel with an ebike battery. Pop off the sides and you have a large number of 12~ wh batteries that don't have any carry on restrictions. I have had trouble using a punch to raise the connectors though without destroying the pcb board it the process
Only brutal acceleration will do.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11673
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Modular Rebuildable Repairable 18650 battery.

Post by spinningmagnets » Aug 27 2016 5:06am

I am really impressed by these...paradigm shift?

User avatar
tiny_n_terrible   100 W

100 W
Posts: 243
Joined: May 19 2013 7:39pm

Re: Modular Rebuildable Repairable 18650 battery.

Post by tiny_n_terrible » Aug 27 2016 10:38am

A similar concept was tried years ago by a motorized bicyclist named Safe.
He used parallel tubes of batteries to achieve the desired voltage and amperage output.
Vibration and inertia from road hazards and bumps caused random open circuits through out the battery pack.
He could not get his battery pack to work reliably.
Maybe you can ?

shawname   1 W

1 W
Posts: 59
Joined: Apr 01 2011 7:45am
Location: Venice, Florida
Contact:

Re: Modular Rebuildable Repairable 18650 battery.

Post by shawname » Aug 27 2016 12:10pm

Thank you for your comment.

My pack is reliable. The neodymium magnets provide button tops for the cells and make it easy to assemble. It's the nylon bolts that provide the compressive strength. A feature of BatteryBlocs is that it can flex and vibrate and not have any spot welds break!

JumperJackFlash   100 W

100 W
Posts: 147
Joined: Dec 05 2015 4:55pm
Location: Los Angeles, CA USA

Re: Modular Rebuildable Repairable 18650 battery.

Post by JumperJackFlash » Aug 27 2016 12:35pm

Really clever idea.

How much strain can the bolts take?

ejonesss   10 kW

10 kW
Posts: 716
Joined: Aug 31 2008 4:21pm

Re: Modular Rebuildable Repairable 18650 battery.

Post by ejonesss » Aug 27 2016 12:44pm

the cells that you sell you say sold with kit purchase.

if i buy a 10 pack kit then am i able to buy 10 cells? or how does that sold with purchase work?

i like your product it looks very good but i will wait until i see if it stays around because i have seen many products come and go and even get taken over by other companies who then sell them from china.

i am glad to see that you are in the united states especially when buying cells because of the hazmat with batteries.
stuff for Even Newer 4 to 24-cell Battery Management System (BMS)
32 lifepo4 cells 16s2p 40138 green cells √
16s2p 40138 based pack built assembled (building electrical equiv to $2000 eonyx system.*

shawname   1 W

1 W
Posts: 59
Joined: Apr 01 2011 7:45am
Location: Venice, Florida
Contact:

Re: Modular Rebuildable Repairable 18650 battery.

Post by shawname » Aug 27 2016 12:51pm

Yes, I stock Panasonic 18650B cells at 3350 mah hours. I build battery packs both spot welded and with BatteryBlocs and so always stock those cells. I sell the cells at a bit over cost as an incentive to purchase BatteryBlocs. You can buy the number of cells it takes to fill your BatteryBlocs order, but I can't afford to sell the cells without a BatteryBlocs order. I order the cells in 1000 cell lots from my supplier in Hong Kong.

Hope this explains it!

shawname   1 W

1 W
Posts: 59
Joined: Apr 01 2011 7:45am
Location: Venice, Florida
Contact:

Re: Modular Rebuildable Repairable 18650 battery.

Post by shawname » Aug 27 2016 12:52pm

JumperJackFlash wrote:Really clever idea.

How much strain can the bolts take?

Hmm, they are nylon bolts rated for 16 foot lbs torque. A 10 pack has four of them. When tightened they clamp the cells tightly, but not so tightly the cells can't be rotated with resistance.

Does this help?

ejonesss   10 kW

10 kW
Posts: 716
Joined: Aug 31 2008 4:21pm

Re: Modular Rebuildable Repairable 18650 battery.

Post by ejonesss » Aug 27 2016 12:58pm

shawname wrote:Yes, I stock Panasonic 18650B cells at 3350 mah hours. I build battery packs both spot welded and with BatteryBlocs and so always stock those cells. I sell the cells at a bit over cost as an incentive to purchase BatteryBlocs. You can buy the number of cells it takes to fill your BatteryBlocs order, but I can't afford to sell the cells without a BatteryBlocs order. I order the cells in 1000 cell lots from my supplier in Hong Kong.

Hope this explains it!

do you mean under cost? because if you sell over cost then you can afford so the only i can think of to not be able to afford is to sell under cost

still it is a very good deal at $4 a piece where as other places sell them at $8 a piece.
stuff for Even Newer 4 to 24-cell Battery Management System (BMS)
32 lifepo4 cells 16s2p 40138 green cells √
16s2p 40138 based pack built assembled (building electrical equiv to $2000 eonyx system.*

JumperJackFlash   100 W

100 W
Posts: 147
Joined: Dec 05 2015 4:55pm
Location: Los Angeles, CA USA

Re: Modular Rebuildable Repairable 18650 battery.

Post by JumperJackFlash » Aug 27 2016 12:59pm

Have the nylon bolts ever snapped during rough riding?

ejonesss   10 kW

10 kW
Posts: 716
Joined: Aug 31 2008 4:21pm

Re: Modular Rebuildable Repairable 18650 battery.

Post by ejonesss » Aug 28 2016 4:46pm

Scottydog wrote:Personally I'm quite impressed! I think the concept of small mini modules makes it easier to maintain good pressure on the connections with the tensioning bolts. Obviously the bolts needed to be plastic, but is the idea that they create a degree of elasticity and keep even pressure? The modular system is great!

I've often thought about 18650 packs, but purchasing complete welded ones for massive capacities seemed daunting.

Personally I think plated copper plates would be more appealing, the steel ones less so, though I guess a degree of stiffness is important? Aluminium perhaps? Would a conductive paste also be good?

I liked the video explanations, only watched one.

Didn't check you page, but to have the full dimensions for each size along with assembled weights would be good also!

awesome job!


magnets do not stick to Aluminium or copper anyone who works with scrap metals knows this it is the easiest to tell if a piece of metal is tin or steel or not.
stuff for Even Newer 4 to 24-cell Battery Management System (BMS)
32 lifepo4 cells 16s2p 40138 green cells √
16s2p 40138 based pack built assembled (building electrical equiv to $2000 eonyx system.*

Post Reply