Show Us Your Homemade Battery Housing

General Discussion about electric bicycles.
User avatar
Luizlife   1 mW

1 mW
Posts: 10
Joined: Aug 19 2017 4:58pm
Location: MA

Re: Show Us Your Homemade Battery Housing

Post by Luizlife » Sep 06 2017 9:26am

So this is my battery plans, my idea is to keep the batteries intact and just use them as they are. Next step is to make the compartments where they will sit in the frame. But first I will reinforce the frame with another vertical bar.

A literal sack of happiness!!
25159b0070bab4471504708363.jpg
Attachments
99759affd4dd47361504705869.jpg
17 of them.
00559b00505daab21504707845.jpg
Another 11" bar will go by the crank to reinforce the frames connecting points.(thanks Amberwolf!!)
00559b00505daab21504707845.jpg (196.34 KiB) Viewed 4401 times
Creating the kobalt power ebike.

User avatar
alsmith   100 kW

100 kW
Posts: 1182
Joined: Dec 03 2010 7:25pm
Location: Northumberland, UK

Re: Show Us Your Homemade Battery Housing

Post by alsmith » Sep 06 2017 1:41pm

More good ideas. I love the diversity of things that people come up with.
My batteries go at the back because my bike has a step-through frame and I can't put anything in that space- I need it to get onto my bike because I can't lift my legs high enough to get over a crossbar. As time has gone on I sometimes now struggle a bit even with the step-through. Panniers on the rear seem to be the best place for me(motor is a big Crystalyte 5300 on the front) but I wish I could use that space under a crossbar.

User avatar
Luizlife   1 mW

1 mW
Posts: 10
Joined: Aug 19 2017 4:58pm
Location: MA

Re: Show Us Your Homemade Battery Housing

Post by Luizlife » Sep 07 2017 8:46pm

augidog wrote:
whereswally606 wrote:A really neat build, smart too. I wonder what the range is? The motorcycle fairing on the bars seems a bit daft though. Well done.

Sent from my ALE-L02 using Tapatalk
thank you.

when i traveled with the gas drive, i carried almost 200 miles of fuel. now i carry about 50 miles, and i use a portion of that generating electricity. the hub gives me an extra 1/2hp to help the 1.5hp engine on steep grades. also, i use the electric and pedals, no gas, to be polite when the situation calls for it. i always arrive home with the same charge i left with.

the scooter fairing doesn't provide any aero benefits, but it will deflect rain past my faceshield if i tuck behind it. now, if by "daft" you mean "poser" I assure you it's about "function." i run full-time lighting, always have, front and rear, with brake light. the reflector headlight fairing has saved my bacon more than once. plus, it's a great home for my dashboard, which started life as a trashcan flip top.
IMG_20160403_131509_hdr.jpg
IMG_20160402_202107.jpg
2540739_l.jpg
apologies for my off topic replies, this is an excellent thread chock full of great ideas.

Hello, I'd like to know more about the Regen braking ( how you did it in details, parts and such) I'd really like to put in on my ebike. Thank you.
Creating the kobalt power ebike.

augidog   10 W

10 W
Posts: 84
Joined: Sep 29 2012 11:49am

Re: Show Us Your Homemade Battery Housing

Post by augidog » Sep 08 2017 1:19am

....
Last edited by augidog on Jan 08 2018 3:33am, edited 1 time in total.

chefkendra   1 mW

1 mW
Posts: 12
Joined: Apr 28 2017 6:50am

Re: Show Us Your Homemade Battery Housing

Post by chefkendra » Sep 08 2017 5:13am

Luizlife wrote:So this is my battery plans, my idea is to keep the batteries intact and just use them as they are. Next step is to make the compartments where they will sit in the frame. But first I will reinforce the frame with another vertical bar.
Very cool. I'm using Kobalt batteries also, at the same time I'm also building a battery pack out of 18650's. I soldered some Kobalt batteries in parallel to add ah and a smaller footprint. Then I made a quick insert in to the bag that came with my kit. Works great, I just slide the batteries in and I'm off. I got the original idea from YouTuber, vuaeco. I actually used three of his ideas so far. His original box was vertical stacks my is a flat stack. These Kobalt batteries were not very expensive, easy to get and so far very reliable. Anyway can't wait to see your finished product. Good luck.
Attachments
temp box 1.jpg
temp batteries solution
Women who build cool stuff...ROCK!

User avatar
Luizlife   1 mW

1 mW
Posts: 10
Joined: Aug 19 2017 4:58pm
Location: MA

Re: Show Us Your Homemade Battery Housing

Post by Luizlife » Sep 08 2017 6:40am

chefkendra wrote:
Luizlife wrote:So this is my battery plans, my idea is to keep the batteries intact and just use them as they are. Next step is to make the compartments where they will sit in the frame. But first I will reinforce the frame with another vertical bar.
Very cool. I'm using Kobalt batteries also, at the same time I'm also building a battery pack out of 18650's. I soldered some Kobalt batteries in parallel to add ah and a smaller footprint. Then I made a quick insert in to the bag that came with my kit. Works great, I just slide the batteries in and I'm off. I got the original idea from YouTuber, vuaeco. I actually used three of his ideas so far. His original box was vertical stacks my is a flat stack. These Kobalt batteries were not very expensive, easy to get and so far very reliable. Anyway can't wait to see your finished product. Good luck.

Yes!! Thank you. That's who it was. (I had forgotten(seen a thumbnail on my YouTube feed)) he makes really great stuff.
93259b2808de98b01504870541.jpg
I can fit the total of 20 batteries
This is how it is currently looking, I added support to the frame, also left a little cubby hole for the controller.
Attachments
54059b281a2a5f361504870818.jpg
The support
Creating the kobalt power ebike.

chefkendra   1 mW

1 mW
Posts: 12
Joined: Apr 28 2017 6:50am

Re: Show Us Your Homemade Battery Housing

Post by chefkendra » Sep 10 2017 10:00am

Oh yeah, that's a smart spot to stick the controller. Very creative project. :)
Women who build cool stuff...ROCK!

User avatar
Luizlife   1 mW

1 mW
Posts: 10
Joined: Aug 19 2017 4:58pm
Location: MA

Re: Show Us Your Homemade Battery Housing

Post by Luizlife » Sep 17 2017 12:42pm

30959beb2a00ab641505669792.jpg
This is how it currently looks like. All made from plywood. I have all of the size and measures correct to the point where the batteries can slide in and out well enough for me.


But I have a question. What should I use the put all of the wood pieces together? Glue, nails etc..?
84459beb3b70e3f81505670071.jpg
As you can see.

There are a lot of separate little pieces.
84459beb3b70e3f81505670071.jpg (230.77 KiB) Viewed 4177 times
Creating the kobalt power ebike.

Hillhater   100 GW

100 GW
Posts: 10826
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Show Us Your Homemade Battery Housing

Post by Hillhater » Sep 17 2017 6:26pm

Luizlife wrote: This is how it currently looks like.
That frame is dangerous !....it WILL break very quickly.
You will also realise by now that your method of battery build has resulted in a 13 kg assembly that contains just 6kg of cells, and 720 Wh of capacity !
This forum owes its existence to Justin of ebikes.ca

litespeed   100 kW

100 kW
Posts: 1415
Joined: Aug 11 2010 4:42pm
Location: St. Peters, Missouri

Re: Show Us Your Homemade Battery Housing

Post by litespeed » Sep 17 2017 10:17pm

Your freaking me out with that frame.....you have to triangulate......squares and rectangles are bad for strength.

As hillhater mentioned.....loose those pack shells and rid your self of that weight.

Please don't ride that bike like it is.....

Tom
I'm married so you know I'm no stranger to pain!

User avatar
amberwolf   100 GW

100 GW
Posts: 29879
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Show Us Your Homemade Battery Housing

Post by amberwolf » Sep 17 2017 11:25pm

Luizlife, while it is possible there will be no problems with the frame design, I think you should re-read this post
https://endless-sphere.com/forums/viewt ... 0#p1316965

Untriangulated, the only thing I can think of that will resist folding stresses is if you put stiff sides on it, that are fastened to the metal frame itself, all along all of the edges of the metal parallelogram.

If the wooden box itself was stiff enough, you might be able to fasten to it, as long as it fully attached to and filling the metal frame (if there are gaps it will allow flex of the frame which will eventually stress and break it).

But either of these things will require you to extend the frame or the box outward so that it is wider than the batteries, so the sides can attach to it.

If you never hit any bumps or potholes, or do any curb hopping, it might not have enough stress to have a problem.

craneplaneguy   10 kW

10 kW
Posts: 783
Joined: Nov 27 2015 9:15am
Location: S.E. Idaho USA

Re: Show Us Your Homemade Battery Housing

Post by craneplaneguy » Sep 18 2017 11:08pm

I can't recall the term for them, but have used them, coarse threaded (for max bit in wood) brass thingies (inserts?) that have a slot to screw then in with a flat blade driver, and they have a machine screw threaded center. So you screw them in the wood, permanent, and then use machine screws to attach whatever. They hold great, I have some of my home built plane in the baggage area, for access to the elevator pushrod.

User avatar
amberwolf   100 GW

100 GW
Posts: 29879
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Show Us Your Homemade Battery Housing

Post by amberwolf » Sep 18 2017 11:42pm

Yes, I have them in the ends of all the signs I recycled to make the wooden deck and seat/cargobox of SB Cruiser. The ones I've got are crappy die-cast ones that are as big around as my pinky, with 1/4"-20 threads inside. But they make smaller ones.

To use them for the edges of the side covers on the battery box, though, you'd still have to extend the box itself past the batteries.

MBikeRider   1 µW

1 µW
Posts: 1
Joined: May 05 2016 11:20am
Location: Hilly San Francisco, California, USA

Re: Show Us Your Homemade Battery Housing

Post by MBikeRider » Oct 25 2017 8:28pm

Wanted to add my 2 pence to the list:

Bike is a 1997 Jamis Aragon with a 48V 15Ah Ping battery. Max Speed is 34 mph on flats with me weighing 200 lbs.

Image
Image

The housing is made of 1 PVC sheet (left side panel), 1 alum. sheet (right side panel), 2" wide flat bar, some cutout alum. sheet rectangles to bend around frame, 1" wide steel flat bar, and alum. angle bar secured together with steel rivet nuts, rivets, and M8 nuts and bolts.

From a design point of view, I spent a lot of time trying to figure out how to make the frame as accessible (especially on the road) as possible with just my Allen wrench set, and I finally found the solution! Two words: Rivet Nuts. They allow me to make a blind threaded hole so parts don't have to be held via nuts and bolts. To demonstrate the serviceability of the frame, it breaks down into 3 groups: panels, left side frame, right side frame. It's held together with 3 nuts and 8 bolts, using pliers or wrench and Allen wrench to reassemble. The main 3 points of contact with the bike frame are the 2 inch wide aluminum flat bars (pain in the ass to cut), with 2 on top and 1 in the rear. The weight of the frame rests on the top two flat bars along with the weight of the battery. I know they shouldn't be used this way, but the rivets holding them to the left side of the frame (right side with bolts) act as pivots to swivel them when disassembling. In total it takes about 10-15 min to take apart, and thankfully I haven't had the need to in a while.

Price-wise ( or Penny-wise :D ), just the metal frame (fasteners not included) cost around $25 in parts at my local Lowe's. As for my panels, my dad's a contractor so I "borrowed" :wink: them from him, but if I had to do without the expensive aluminum and PVC sheets, I'd just use Coroplast instead and 2-ply that on both sides (around $20 for a 4 x 8 ft sheet). What surprised me was how expensive rivet nuts and bolts cost plus shipping: around $27 on Fastenal :o ! Although, I have to say it did include the parts necessary to use a rivet nut in the first place. The rivet nuts were also annoyingly difficult to use right.

As you can probably tell, it's more a function over form build, but it gets the job done :D . The right side panel is aluminum because the bike leans left when locked up and the sun had caused the previously PVC right side panel to warp :( . From the front, there's nothing bracing the front of the panels which causes it to bend out a bit there.

Vibration and bumps-wise, the battery is suspended with wire to prevent it from smashing the wires underneath, but I haven't figured out how to hold the controller in place, causing it to rub against the right panel on bumpy roads.

Here's my baby in whole :D :
Image
Last edited by MBikeRider on Oct 25 2017 9:46pm, edited 1 time in total.
1997 Jamis Aragon hybrid with 48V 15Ah Ping Battery and 1680W Cyclone Motor. Max Speed: 34 MPH.

[0] days without an accident

augidog   10 W

10 W
Posts: 84
Joined: Sep 29 2012 11:49am

Re: Show Us Your Homemade Battery Housing

Post by augidog » Oct 25 2017 9:31pm

....
Last edited by augidog on Jan 08 2018 3:33am, edited 1 time in total.

felix991   1 mW

1 mW
Posts: 19
Joined: Sep 26 2017 6:48am
Location: DFW, Texas, USA

Re: Show Us Your Homemade Battery Housing

Post by felix991 » Oct 31 2017 11:44pm

I have been a lurker for years but I finally registered because I am building two more. A Qulbix 76r and a EEB Endurobike (the chinese stealth knockoff) But since I never posted a photo of my last one, this looks like a good as any place to start.

I found that bag on ebay, at the time I didnt even know who em3ev was. But I built this bike from scratch. It started as a GT Aggressor 2.0 I found of Craiglist for 200 bucks and I had never built a electric bike before so there were several iterations before this final photo.

This is a 52V20AH battery with a BMC 6T motor. I got the Marzocchi's off ebay for 250 and had a local bike shop build me a new DH rim after I ruined the stock Suntour forks and rim. I also went thru several back tires and tubes before I landed on this specialized ground control and that tire still amazes me. I have run it over glass and nails sharp rocks and even flat for several miles and it's still good to go. The front tire is a Maxxis Holly Roller and I just bought it cause it looked cool and I will never run another type for as long as I ride. That tire runs perfect on all my regular street trail paths I take and both of them have over 1800 miles on them now.

My hobbies have been elseware the last few years but I still go ride everyday at dusk and usually one big trip every few weekends somewhere in the DFW area. There are 100's of miles of bike trials here. But a few weeks ago my planetary gear in the BMC finally gave out and so now I am back on bikes. I have my floor littered with boxes and parts and I will make some posts on my findings. As I stated I am building one quilbix 76r with all the good stuff and one EEB Chinese knock off frame with all 'reliable' but cheap parts. They both will be powered with the EDGE 1500 watt hub motor. I may go to a MXUS later. I just dont think I will need it after the reviews on the EDGE. I am old and my young dirt bike days have destroyed most of my body parts so I dont ride hard anymore. I just like to ride. The 76r is for me the EEB is for my friend. He is a cheapskate so I thought I would make a project out of it and document the differences between a ~1100 and ~2500 build

I get about 55 miles on a charge with my current setup and have been averaging 17-19 watt hours it tops out at about 31mph. But now that I am building these two new ones all the sudden now all my friends want ebikes too so I was here looking at battery box options for those that just want to convert their MTB. I really liked the little triangle pack in the fat bike. thanks for the idea. I never would have thought to cut PVC in half and flatten it out. Genius.
Attachments
IMG_5451.jpg

User avatar
Luizlife   1 mW

1 mW
Posts: 10
Joined: Aug 19 2017 4:58pm
Location: MA

Re: Show Us Your Homemade Battery Housing

Post by Luizlife » Nov 04 2017 6:56pm

What do you guys think of the almost finished product?

I still have to add the car horn to it..

I've already put over 70 miles on it. There is nothing wrong as I can see. I get a total of 30 mile range on one full charge.

Total price is $584
Attachments
IMAG0615_resized.jpg
IMAG0615_resized.jpg (238.03 KiB) Viewed 3787 times
IMAG0616_resized.jpg
IMAG0616_resized.jpg (224.49 KiB) Viewed 3787 times
IMAG0617_resized.jpg
IMAG0617_resized.jpg (224.68 KiB) Viewed 3787 times
IMAG0618_resized.jpg
IMAG0618_resized.jpg (237.6 KiB) Viewed 3787 times
IMAG0619_resized.jpg
IMAG0619_resized.jpg (216.56 KiB) Viewed 3787 times
IMAG0621_resized.jpg
IMAG0621_resized.jpg (215.41 KiB) Viewed 3787 times
IMAG0622_resized.jpg
IMAG0622_resized.jpg (213.13 KiB) Viewed 3787 times
IMAG0623_resized.jpg
IMAG0624_resized.jpg
IMAG0624_resized.jpg (221.71 KiB) Viewed 3787 times
IMAG0625_resized.jpg
IMAG0625_resized.jpg (215.21 KiB) Viewed 3787 times
IMAG0626_resized.jpg
IMAG0627_resized.jpg
Chain tension adjuster
Creating the kobalt power ebike.

duerr_joe@yahoo.com   100 µW

100 µW
Posts: 9
Joined: Apr 22 2016 8:24pm

Re: Show Us Your Homemade Battery Housing

Post by duerr_joe@yahoo.com » May 18 2018 11:36am

36 volt 27.2 amp hours 10s8p pack. compact and light weight. NO welding or soldering. A circuit board at the bottom and top makes changing an individual battery easy.
Attachments
0503ws2.jpg
0503ws2.jpg (176.74 KiB) Viewed 3061 times

Bobw   10 mW

10 mW
Posts: 24
Joined: Jun 20 2017 4:30pm
Location: Edmonton, Alberta

Re: Show Us Your Homemade Battery Housing

Post by Bobw » May 19 2018 1:42pm

Here’s what I came up with when doing my MTB conversion last year.... a box made from 4mm acrylic sheet, 2 sections, one for the 96 cell battery pack, the other for the controller and wiring connections.

I was warned that acrylic is not the best because of cracking with vibration and stress but so far no issues, except when I dropped the side cover on concrete during assembly. All in all it has proven to be a pretty good solution on how to mount a battery onto the bike frame.

An added bonus to using this method was the ability to illuminate the box for night riding. Makes my ride a little unique.

If anyone would like to see more details, I shot some video of my conversion project including the assembly of the box.
Attachments
EE01A594-940C-40A4-AF46-D5F445AE0EF7.jpeg
0A04874F-EC89-4D94-B11A-7153AAA994F7.jpeg
02AB0C3D-263F-4C23-9B23-6FCC7F55A85C.jpeg
A0AB2713-B2B5-4EA4-893E-847DD49C8E0B.jpeg
A0AB2713-B2B5-4EA4-893E-847DD49C8E0B.jpeg (79.63 KiB) Viewed 2994 times

User avatar
lowrider13   100 µW

100 µW
Posts: 9
Joined: Dec 06 2013 5:34am
Location: Perth - Mighty Mighty West

Re: Show Us Your Homemade Battery Housing

Post by lowrider13 » May 20 2018 8:57am

My homemade battery housing - 3.5mm perspex with double layer on the base for strength. Held on with 3 x 12mm u-bolts.
Holds my 14S19P PF EM3EV pack. Used to have controller inside enclosure (note vents on the rear. Has air-intake built into bottom of enclosure)
30A Controller was moved next to crank - (dont recommend for off roading!!) Good for stealth though.
charge port built into back and key switch on the top.
Motor is 6T Mac.
IMG_1800-2.jpg
IMG_1800-2.jpg (106.54 KiB) Viewed 2957 times
IMG_1793-2.jpg
IMG_1793-2.jpg (101.21 KiB) Viewed 2957 times
IMG_1799-2.JPG
IMG_1799-2.JPG (106.42 KiB) Viewed 2957 times
IMG_1801-2.jpg
IMG_1801-2.jpg (108.81 KiB) Viewed 2957 times
* 2013 Giant Yukon - Version 5 Mac 8T + Cellman 50V (Samsung30Q) Triangle pack (17.5AH) + Infineon Clone 30A (was magic pie 3 - converted to external controller)
* 2014 Merdia Matts 40 + Bafang 750W 8fun Mid-drive - 48V 10AH LiFePO4 (was Mac 6T + 40A Infineon)
* Stealth FUTR Beta - MXUS + 20S powered

User avatar
John and Cecil   1 kW

1 kW
Posts: 496
Joined: Mar 14 2018 7:26pm

Re: Show Us Your Homemade Battery Housing

Post by John and Cecil » May 20 2018 9:29am

Bobw wrote:
May 19 2018 1:42pm
Here’s what I came up with when doing my MTB conversion last year.... a box made from 4mm acrylic sheet, 2 sections, one for the 96 cell battery pack, the other for the controller and wiring connections.

I was warned that acrylic is not the best because of cracking with vibration and stress but so far no issues, except when I dropped the side cover on concrete during assembly. All in all it has proven to be a pretty good solution on how to mount a battery onto the bike frame.

An added bonus to using this method was the ability to illuminate the box for night riding. Makes my ride a little unique.

If anyone would like to see more details, I shot some video of my conversion project including the assembly of the box.
Are those solderless battery terminals? I have been looking into some other ones and those look pretty heavy duty. The ones I saw have the plastic caps slide over the ends but yours appear to be in blocks which are then bolted together. Do you have any issues with them losing contact? Do you recommend using them and where did you get them? Thanks you!

Bobw   10 mW

10 mW
Posts: 24
Joined: Jun 20 2017 4:30pm
Location: Edmonton, Alberta

Re: Show Us Your Homemade Battery Housing

Post by Bobw » May 20 2018 12:04pm

http://www.batteryblocs.com/

Used 8P 12S on my bike. Seems to work well so far. I don’t run a BMS on my pack and do a split pack charge when balancing is required.

User avatar
John and Cecil   1 kW

1 kW
Posts: 496
Joined: Mar 14 2018 7:26pm

Re: Show Us Your Homemade Battery Housing

Post by John and Cecil » May 20 2018 12:21pm

Bobw wrote:
May 20 2018 12:04pm
http://www.batteryblocs.com/

Used 8P 12S on my bike. Seems to work well so far. I don’t run a BMS on my pack and do a split pack charge when balancing is required.
Very cool, thank you for the link. :) I like how they bolt together. I would think if they ever did start intermittently lose connection on bumps a quick retightening of the bolts would fix it :) I also like the concept because after your batteries die over time you can upgrade to newer batteries and keep your housing, etc.

User avatar
amberwolf   100 GW

100 GW
Posts: 29879
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: Show Us Your Homemade Battery Housing

Post by amberwolf » May 20 2018 11:22pm


User avatar
tomjasz   10 GW

10 GW
Posts: 4223
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: Show Us Your Homemade Battery Housing

Post by tomjasz » May 21 2018 1:03am

John and Cecil wrote:
May 20 2018 12:21pm
Bobw wrote:
May 20 2018 12:04pm
http://www.batteryblocs.com/

Used 8P 12S on my bike. Seems to work well so far. I don’t run a BMS on my pack and do a split pack charge when balancing is required.
Very cool, thank you for the link. :) I like how they bolt together. I would think if they ever did start intermittently lose connection on bumps a quick retightening of the bolts would fix it :) I also like the concept because after your batteries die over time you can upgrade to newer batteries and keep your housing, etc.
Neodymium magnets dislike heat, as long as the pack never gets a hot cell or 3, all is well. Batteryblocs are quite large and take up space. But they do work. I like the V2 Vruzend for a more compact solderless build, and no magnets.

Bob’s box rocks! I like it!
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.