How to use a 250W front hub motor with an aluminium for and survive?

General Discussion about electric bicycles.
Post Reply
hrc   100 µW

100 µW
Posts: 8
Joined: Jan 17 2020 8:10pm

How to use a 250W front hub motor with an aluminium for and survive?

Post by hrc » Jan 22 2020 4:09pm

Yes, the common advise is NEVER to use an aluminum fork when using a front hub motor.
But on the other hand there are hundred of thousands of ebikes with aluminum forks and front hub motors (Vanmoof and many others).
So my question is, what would be the the key concepts to consider if you want to use and aluminum for with a 250W front hub motor?
  • Special torque torque arms?
  • Custom made aluminium forks for front hub motors?
  • Use special washers?
  • Limit the max power of the motor?
  • Combination of above?
Has anyone been able to use a small 250W motor with a aluminium fork with no problems? Any tips?
Thanks for your help!

User avatar
amberwolf   100 GW

100 GW
Posts: 29035
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: How to use a 250W front hub motor with an aluminium for and survive?

Post by amberwolf » Jan 22 2020 4:31pm

if youre up for some reading, threads in these lists have answers to your questions. should be obvious by title which are relevant:

search.php?keywords=alloy*+fork*+motor* ... mit=Search

search.php?keywords=alu*+fork*+motor*&t ... mit=Search

there's also info in these but most aren't completely relevant and/or dont' have all the info within them that you want:
search.php?keywords=front+hub+motor*&te ... mit=Search

docw009   100 kW

100 kW
Posts: 1237
Joined: Aug 02 2015 7:43am
Location: Chicago area suburbs.

Re: How to use a 250W front hub motor with an aluminium for and survive?

Post by docw009 » Jan 22 2020 8:25pm

Ive had a 250W Q100H motor on my 20' minivello for two years. Alloy fork. I have torque arms on both sides, one home made and the other store bought. I'm running it off 36V and a 20A controller, so it can peak at 600-700 watts briefly.

I marked the nuts with a red pen, and they haven't moved. Nonetheless, it worries me. In one picture, you can see there was just enough thread to engage all the the hub nut.

This winter, it comes off and I will drive the rear wheel instead with a mid drive.
torqu1.jpg
torqu1.jpg (76.35 KiB) Viewed 768 times
torque2.jpg
torque2.jpg (80.31 KiB) Viewed 768 times

markz   100 GW

100 GW
Posts: 8574
Joined: Jan 09 2014 11:38pm
Location: Alberta Canada

Re: How to use a 250W front hub motor with an aluminium for and survive?

Post by markz » Jan 22 2020 8:42pm

I am using a yescomusa direct drive 9c clone on the front, its 36V26A using ONE torque arm! T.A. is 1.5"x4"x1/4" steel flat stock, using an angle grinder I cut out the axle notch, then a small notch where the hose clamp fits in nicely and secures it tot he frame fork.
I recently inspected the front alum fork dropouts, they are fine.
btw I am fat at 375lbs, its stretched out fat so dont make no fat jokes.

User avatar
dogman dan   100 GW

100 GW
Posts: 35411
Joined: May 17 2008 12:53pm
Location: Las Cruces New Mexico USA

Re: How to use a 250W front hub motor with an aluminium for and survive?

Post by dogman dan » Jan 25 2020 8:21am

The first key thing for an alloy fork front motor, is you need the C washers. You must have an inner washer so the nut does not bear on the shoulder of the fork ( lawyer lips). Without this, just tightening the nut will crack the fork.

Then two decent torque arms. If its a shock fork, then you need the larger, more adjustable ones from Grin Technologies.

Weak motors do help, even steel forks can be wrecked by enough power. But 1000w setups, 500w rated motors running 20 amps, can be done if the washers and TA's are ok.

User avatar
motomech   1 GW

1 GW
Posts: 3383
Joined: Sep 11 2010 12:21am
Location: Punta Cana Baja Mexico

Re: How to use a 250W front hub motor with an aluminium for and survive?

Post by motomech » Jan 25 2020 5:37pm

Yes, above exactly.
Here's a tip;
The C-washer has to sit flat against the fork ear.
If any part of the special washer contacts the ridge of the "Lawyer's Lips", one can go straight in with the flat side of a standard Dremel abrasive disc. It's exactly the same size of the C-washer and will clean-up the surface nicely.
Motomech

'03 Rocky Mountain Edge 2WD 260 Q100H frt and Ezee V1 rear 2 Elifebike 20A & 25A 9-FET controllers 12S/10Ah Multistar Lipo rear 4Ah Turnigy frt Luna Cyclops Extra lite Alex 24DM rims, Crazy Bobs run ghetto tubeless. 25 mph. Mean Well HLG-320H-54A
https://endless-sphere.com/forums/viewt ... =3&t=83430
'07 GT Idive 4 4.0, Q100C 201 14S LiPoly elifebike 9-FET 20A controller. 23 MPH.
https://endless-sphere.com/forums/viewt ... 4#p1378484

User avatar
Hwy89   1 kW

1 kW
Posts: 431
Joined: Mar 03 2013 9:52pm
Location: Northern Arizona

Re: How to use a 250W front hub motor with an aluminium for and survive?

Post by Hwy89 » Jan 25 2020 10:31pm

Where do you find the "C" washers for sale?
Installed a motor today on a fork with the most pronounced "lawyers lips I've ever seen. This evening reading this thread decided I'd better get C washers.

markz   100 GW

100 GW
Posts: 8574
Joined: Jan 09 2014 11:38pm
Location: Alberta Canada

Re: How to use a 250W front hub motor with an aluminium for and survive?

Post by markz » Jan 25 2020 10:33pm

Only one custom steel t.a.

Clipboard01.jpg
Clipboard01.jpg (40.67 KiB) Viewed 666 times

User avatar
amberwolf   100 GW

100 GW
Posts: 29035
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: How to use a 250W front hub motor with an aluminium for and survive?

Post by amberwolf » Jan 25 2020 10:42pm

Hwy89 wrote:
Jan 25 2020 10:31pm
Where do you find the "C" washers for sale?
https://www.google.com/search?newwindow ... +C+washers