Post by rg12 » Apr 12 2019 6:51pm

I have a Hakko Presto which I use to solder up to 8AWG and that little thing does it amazing.
I would like to hear about any recommendations for quality yet affordable soldering irons/stations for a higher power setup to solder 5AWG wires.
Mind that the Hakko Presto is the best soldering iron I ever used and it's super cheap ($30-$50).

major   10 kW

10 kW
Posts: 808
Joined: Mar 10 2013 10:12am
Location: NW Ohio, USA

Re: Recommended Soldering Iron for 5AWG?

Post by major » Apr 12 2019 7:23pm

Ever consider a torch?

john61ct   100 GW

100 GW
Posts: 5053
Joined: Dec 18 2018 2:06pm

Re: Recommended Soldering Iron for 5AWG?

Post by john61ct » Apr 12 2019 8:14pm

or crimping?

Ohbse   10 kW

10 kW
Posts: 880
Joined: Dec 26 2013 5:15pm
Location: Auckland, New Zealand

Re: Recommended Soldering Iron for 5AWG?

Post by Ohbse » Apr 12 2019 10:19pm

Best soldering iron for wiring that size is no soldering iron, it's just not the right technique for connections at that scale.

Best option is to invest in a hydraulic crimper - they can be had pretty cheaply from ebay etc. I love mine.

User avatar
tomjasz   10 GW

10 GW
Posts: 4223
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: Recommended Soldering Iron for 5AWG?

Post by tomjasz » Apr 12 2019 11:18pm

Get The TS100 Digital OLED Programmable Soldering Iron is an internal heating intelligent CNC soldering iron.

Check out the reviews. A real winner!
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

User avatar
dogman dan   100 GW

100 GW
Posts: 35593
Joined: May 17 2008 12:53pm
Location: Las Cruces New Mexico USA

Re: Recommended Soldering Iron for 5AWG?

Post by dogman dan » Apr 13 2019 7:48am

Big fat tip iron will do, even low wattage, if the tip is fat enough. But personally, I'd go to crimps or lugs by 5g.

User avatar
spinningmagnets   100 GW

100 GW
Posts: 11611
Joined: Dec 21 2007 10:27pm
Location: Ft Riley, NE Kansas

Re: Recommended Soldering Iron for 5AWG?

Post by spinningmagnets » Apr 13 2019 8:41am


rg12   100 kW

100 kW
Posts: 1278
Joined: Jul 26 2014 4:22pm

Re: Recommended Soldering Iron for 5AWG?

Post by rg12 » Apr 14 2019 9:19am

Thanks guys, I guess I will go with crimping then

User avatar
Schlafmutze   10 W

10 W
Posts: 71
Joined: Apr 23 2014 4:53pm

Re: Recommended Soldering Iron for 5AWG?

Post by Schlafmutze » Apr 14 2019 3:23pm

I solder 4 AWG with a weller WS81, using fat tip.
A TS100 with a fat tip will work too.

That 80w Iron is enough to solder long pieces of AWG4 onto my BMS PCB even.

rg12   100 kW

100 kW
Posts: 1278
Joined: Jul 26 2014 4:22pm

Re: Recommended Soldering Iron for 5AWG?

Post by rg12 » Apr 15 2019 4:35am

Schlafmutze wrote:
Apr 14 2019 3:23pm
I solder 4 AWG with a weller WS81, using fat tip.
A TS100 with a fat tip will work too.

That 80w Iron is enough to solder long pieces of AWG4 onto my BMS PCB even.
Good to know, thanks alot :)

User avatar
tomjasz   10 GW

10 GW
Posts: 4223
Joined: Mar 29 2014 1:45pm
Location: Out riding, MN USA
Contact:

Re: Recommended Soldering Iron for 5AWG?

Post by tomjasz » Apr 19 2019 10:28pm

TS100

A couple of optional tips and bob’s yer uncle.
Thanks Justin_le we're here thanks to you. All the best to the mods for their tireless work keeping it on an even keel.

john61ct   100 GW

100 GW
Posts: 5053
Joined: Dec 18 2018 2:06pm

Re: Recommended Soldering Iron for 5AWG?

Post by john61ct » Apr 20 2019 2:37pm

Schlafmutze wrote:I solder 4 AWG with a weller WS81, using fat tip.
A TS100 with a fat tip will work too.

That 80w Iron is enough to solder long pieces of AWG4 onto my BMS PCB even.
https://youtu.be/83STpUXHilk

Just love this guy!