Recent house destroying Ebike battery fire in Sydney and a recall on defective Ezee batteries
https://www.smh.com.au/business/consume ... .html?btis
Apparently Ezee are blaming the LG cells for a defect ?

Re: Ezee battery fire & recall

Posted: Apr 30 2019 3:46am
by district9prawn
Hillhater wrote:
Apr 28 2019 5:20am
Apparently Ezee are blaming the LG cells for a defect ?
And looks like LG deny everything. I don't recall reading that in article on the day it was published. I only noticed it today?

Re: Ezee battery fire & recall

Posted: May 28 2019 4:56pm
by Matador
Faulty BMS also likely ... To allow overcharging a cell group to a point of unstability. I'm thinking, at leas 4.4V...

Re: Ezee battery fire & recall

Posted: May 28 2019 4:58pm
by billvon
Matador wrote:
May 28 2019 4:56pm
Faulty BMS also likely ... To allow overcharging a cell group to a point of unstability. I'm thinking, at leas 4.4V...
Or a puncture. Or an internal short. A little early to be deciding it's overcharge.

Re: Ezee battery fire & recall

Posted: May 28 2019 6:23pm
by Hillhater
I assume Ezee did do some basic inspection and checks to eliminate obvious faults before they issued a recall , let alone finger a reputable cell manufacturer like LG.

Re: Ezee battery fire & recall

Posted: May 28 2019 8:41pm
by Matador
billvon wrote:
May 28 2019 4:58pm
Matador wrote:
May 28 2019 4:56pm
Faulty BMS also likely ... To allow overcharging a cell group to a point of unstability. I'm thinking, at leas 4.4V...
Or a puncture. Or an internal short. A little early to be deciding it's overcharge.
Internal short also good possibility. But puncture ? The battery was left charging ovenight, left unattended. So puncture not impossible but seems unlikely.

Maador

Re: Ezee battery fire & recall

Posted: May 28 2019 9:20pm
by neptronix
I love how she just put a new battery on the bike and kept riding...