I am wondering why Sony provides the attached JPG of their VTC5 cell dimensions and yet when I communicate with cell suppliers they say that the anode top is absolutely flush with the shrink wrap edge. Can anyone shed more light on this question?
Attachments
18650 dimension SonyVTC5.jpg
18650 dimension SonyVTC5.jpg (30.67 KiB) Viewed 1485 times

User avatar
e-beach   1 GW

1 GW
Posts: 3362
Joined: Jan 10 2012 9:48pm
Location: Any Los Angeles area beach I am at. Or Santa Monica or possibly the south bay beaches.

Re: actual 18650 cell anode end dimensions

Post by e-beach » Mar 03 2016 7:48pm

Probably because the picture is not titled properly. Go with what your vendors say. They are looking at the cells they have.

Edit: I just looked at the picture again, if you look at the .02 gap measurement at the bottom of the picture, it relates to the + or - tollerences at the top of the picture.

:D
Favorite Quotes:
"This is L.A., sugar. There is no 'over the top." Chris Erskine
"At a certain point the entropy wins." Maria Helena Braga

Current Build: ProFlex 757 Expert full suspension. Yescomusa 36v 800w Rear DD, upgraded 10AWG solid core through axle phase wires. 15ah Headway, 1000+ cycles, 80% DOD 30A Tronsung controller.

Past: Trek 4500 Yescomusa 36v 800w front DD.
Liahona, Yescomusa 36v 800w generic front DD.
1992 Trek 800, Yescomusa 800w 36v front DD.

User avatar
bowlofsalad   1 MW

1 MW
Posts: 1540
Joined: Feb 01 2013 10:28pm
Location: Midwest, USA

Re: actual 18650 cell anode end dimensions

Post by bowlofsalad » Mar 03 2016 8:10pm

Great question and one I've sort of asked myself.

So far as I know there are two types of tops, button and flat. It honestly looks like that is an image of a protected cell or something, on the left or top of that cell there is a smaller segment of rectangle which might be a protection PCB, maybe a few MM thick. I could be wrong though. However, it might be that these cells often start off as flat top cells and then the button is often added one another or another either for some form of more ideal contact in certain situations or as part of the protection PCB, probably more to it than I imagine.

Sorry to say, my answer is likely primarily speculative.

https://www.google.com/?gws_rd=ssl#q=fl ... +top+18650

kenkad   100 W

100 W
Posts: 193
Joined: Oct 12 2009 9:36pm
Location: Union Grove, AL, USA

Re: actual 18650 cell anode end dimensions

Post by kenkad » Mar 03 2016 8:15pm

bowlofsalad,
A button top is just as it says. Primarily designed for flashlights, etc., or cell holders. And, NO, the tolerance on the cell has nothing to do with the 0.2mm at the top.

I personally think that the 0.2mm is consistent with the thickness of the isolation rings that are available. Put that on the anode end and then the anode top is flush with the top of the isolation pad. I would like some confirmation from people who know and not be guessing.

User avatar
bowlofsalad   1 MW

1 MW
Posts: 1540
Joined: Feb 01 2013 10:28pm
Location: Midwest, USA

Re: actual 18650 cell anode end dimensions

Post by bowlofsalad » Mar 03 2016 8:25pm

I communicate with cell suppliers they say that the anode top is absolutely flush with the shrink wrap edge
I wouldn't be surprised if I misunderstand, but I am saying that when they say this they might be referring to a flat top cell, the picture of the cell looks like a button top cell and a cell seems like it can sometimes come in either version.

kenkad   100 W

100 W
Posts: 193
Joined: Oct 12 2009 9:36pm
Location: Union Grove, AL, USA

Re: actual 18650 cell anode end dimensions

Post by kenkad » Mar 03 2016 8:36pm

Just received this from a 18650 supplier (will remain unnamed).

*****************************************************************************************
And you asked about Samsung, not Sony.
I mentioned in my email* it's manufacturer and model specific. *The
Samsung models I have have no dimension specified there and that is also
shown in real life measuring with calipers. Panasonic and Sony do indeed
protrude a little bit.
*****************************************************************************************

So, go figure, and, there is supposed to be a standard?

EDIT:
The question is now is this also the case with the Sanyo that is now Panasonic?
I believe I may go with the Sanyo GA.

User avatar
Grizzl-E   100 W

100 W
Posts: 206
Joined: Jun 01 2015 9:57pm
Location: Manitoba, Canada

actual 18650 cell anode end dimensions

Post by Grizzl-E » Mar 03 2016 9:06pm

Had these on my desk so here are some samples. Sorry I don't have the ones in the op.
ImageUploadedByTapatalk1457056684.400309.jpg
ImageUploadedByTapatalk1457056304.149748.jpg
ImageUploadedByTapatalk1457056285.928802.jpg
ImageUploadedByTapatalk1457056192.201376.jpg
Brown are LG HG2's. Purple are Panasonic 29e's, the group of them has paper spacers on already. Red are laptop cells, possibly Sanyo. All are unprotected. You can see they are all very close and the tops roughly line up with the shrink wrap.

Edit: the 0.2mm in the diagram is likely filled by the squishyness for lack of a better term of the integrated isolator and shrink wrap. These are flat tops btw.
Only brutal acceleration will do.

Hillhater   100 GW

100 GW
Posts: 10970
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: actual 18650 cell anode end dimensions

Post by Hillhater » Mar 03 2016 9:30pm

Jeez !.... :shock: ...I hope those are not metal callipers ?
Fact. Cell length varies depending on the maker, model, protected or non protected, and spec of the cell ..( all 18650)
Fact ...many cells can be bought with either "flat top". (Flush) , " Button top" , tab, etc etc configuration.
Precise dimensions can be found by searching the flashlight or Vape test sites
This forum owes its existence to Justin of ebikes.ca

User avatar
Grizzl-E   100 W

100 W
Posts: 206
Joined: Jun 01 2015 9:57pm
Location: Manitoba, Canada

Re: actual 18650 cell anode end dimensions

Post by Grizzl-E » Mar 03 2016 9:44pm

Lol yes they are metal! I was very careful. 3.8 volts is also a lot less than I usual have to work with so I wasn't too worried :)
Only brutal acceleration will do.

kenkad   100 W

100 W
Posts: 193
Joined: Oct 12 2009 9:36pm
Location: Union Grove, AL, USA

Re: actual 18650 cell anode end dimensions

Post by kenkad » Mar 03 2016 10:31pm

WOW, a vape test site! But you have to 18!

Punx0r   100 GW

100 GW
Posts: 5513
Joined: May 03 2012 8:16am
Location: England

Re: actual 18650 cell anode end dimensions

Post by Punx0r » Mar 04 2016 6:56am

The diagram looks like a button top cell, but 0.2mm is no where near tall enough. I suspect it's a maximum or nominal height of the flat top cap.