Battery List

Batteries, Chargers, and Battery Management Systems.
Post Reply
markz   100 GW

100 GW
Posts: 9796
Joined: Jan 09 2014 11:38pm
Location: Alberta Canada

Battery List

Post by markz » Aug 01 2015 9:21pm

Here is a list I did, from various sources.

If there is a mistake, just say what it is and I will double check the info and change it.
Book1.pdf

User avatar
Nobuo   10 kW

10 kW
Posts: 839
Joined: Nov 21 2014 3:38am
Location: Madrid

Re: Battery List

Post by Nobuo » Aug 03 2015 12:02pm

Very worked compilation. Thank you for your highly appreciated help to this community :o

Samsung 29E are more like 7A max.

It would be great if you add the chemistry specification, like NMC, NCA, etc
* Lithium + Air = Fire * <-----> ** Lithium + Chemical-Additives + Air = ZERO Fire **
<Battery and EV works>
https://facebook.com/evmadrid1
<Battery building resources>
http://www.endless-sphere.com/forums/vi ... 14&t=68005

markz   100 GW

100 GW
Posts: 9796
Joined: Jan 09 2014 11:38pm
Location: Alberta Canada

Re: Battery List

Post by markz » Aug 11 2015 11:55pm

You are welcome Nobuo.

I made this list because I kept having to go to several difference sources to find the discharge rates for different cells. Thats all I am really interested in rather then the chemistry type, but perhaps they are related. As far as the chemistries go, I think if its not listed its whatever the above one is. I looked at it and can only assume thats what I did because I was working from several different hand written notes and different web pages.

Yes its all 18650 because thats what I am looking at buying.

Be cool to have a way for users to add info and get more details, more variety of types. Guess thats what wiki is for.

markz   100 GW

100 GW
Posts: 9796
Joined: Jan 09 2014 11:38pm
Location: Alberta Canada

Re: Battery List

Post by markz » Aug 13 2015 5:39pm


User avatar
Nobuo   10 kW

10 kW
Posts: 839
Joined: Nov 21 2014 3:38am
Location: Madrid

Re: Battery List

Post by Nobuo » Aug 13 2015 8:55pm

mother of god :o

awesome compilation, now samsung 29E are slightly over its discharge rate :lol: , it is close to 7A max, at 10A they perform really bad.

So you will unite this with your compilation, or everything was there yet?

really thank you for sharing!!
* Lithium + Air = Fire * <-----> ** Lithium + Chemical-Additives + Air = ZERO Fire **