Thread for new battery breakthrough PR releases

Batteries, Chargers, and Battery Management Systems.
Hillhater   100 GW

100 GW
Posts: 10808
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Thread for new battery breakthrough PR releases

Post by Hillhater » Sep 22 2019 7:40pm

Ultra fast charing cell.....or is it a capacitor ?...or just more vaporware ?
Zap Go carbon C-ion cell.
https://www.businesswire.com/news/home/ ... c-Vehicles
This forum owes its existence to Justin of ebikes.ca

furcifer   10 kW

10 kW
Posts: 617
Joined: Dec 21 2018 12:36pm

Re: Thread for new battery breakthrough PR releases

Post by furcifer » Oct 24 2019 2:50pm

"First fully rechargeable carbon dioxide battery with carbon neutrality"

Lithium-carbon dioxide batteries are attractive energy storage systems because they have a specific energy density that is more than seven times greater than commonly used lithium-ion batteries. However, until now, scientists have not been able to develop a fully rechargeable prototype, despite their potential to store more energy.


https://www.sciencedaily.com/releases/2 ... 101331.htm

I'm not sure if this has been posted here or not. 7 times the energy density is a game changer if they can get the charge cycles out of the chemistry.

Punx0r   100 GW

100 GW
Posts: 5513
Joined: May 03 2012 8:16am
Location: England

Re: Thread for new battery breakthrough PR releases

Post by Punx0r » Oct 24 2019 5:01pm

The article suggests they have demonstrated 500 cycles? Although "charge-recharge" cycles is an odd way of stating it.

User avatar
Honk   100 W

100 W
Posts: 226
Joined: Oct 10 2011 3:31pm

Re: Thread for new battery breakthrough PR releases

Post by Honk » Nov 20 2019 5:32am

Any technical oddity in press releases if often a sign of bullshit and wapor ware.
The press release itself is just a fraud and the intent is raising investment capital.
Efficiency is king!

User avatar
fechter   100 GW

100 GW
Posts: 14714
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: Thread for new battery breakthrough PR releases

Post by fechter » Nov 20 2019 9:21am

From this article:
https://www.forbes.com/sites/alanohnsma ... 5a17e4157a
Nikola Motor, the Phoenix-based startup that wants to disrupt trucking with futuristic electric semis powered by hydrogen, says it has developed a new type of battery cell with double the energy density, only 40% of the weight and half the cost of current lithium-ion batteries used in Teslas and other consumer-market electric vehicles.

But it’s not providing many details for now, and public demonstrations won’t happen for about 10 months.

Battery packs using the new cells, which don’t use nickel, cobalt and other metals typically found in 2170 lithium-ion cells favored by Tesla, could boost range for current electric passenger cars from 300 miles per charge to as much as 600 miles with “little or no increase to battery size and weight,” the company said. Nikola has subjected its cells to heavy-duty testing and says that charging and depleting them “over 2,000 times has shown acceptable end-of-life performance.”
and
Many years of undelivered promises created considerable skepticism among auto engineers and executives, some of whom grouse about “liars, damn liars and battery suppliers.”
and maybe it's an investor scam:
Nikola has raised about $500 million to get its hydrogen fuel cell trucks into production, gaining a $3 billion valuation, and needs to raise considerably more to also build its own network of hydrogen fuel stations to power them.
We'll see........
"One test is worth a thousand opinions"

User avatar
TheBeastie   1 MW

1 MW
Posts: 1993
Joined: Jul 28 2012 12:31am
Location: Melbourne Australia

Re: Thread for new battery breakthrough PR releases

Post by TheBeastie » Nov 20 2019 11:29am

fechter wrote:
Nov 20 2019 9:21am
From this article:
https://www.forbes.com/sites/alanohnsma ... 5a17e4157a

We'll see........
There are new Hydrogen fuelcell projects being launched every other day for large vehicles like buses and trains and even ships.
Mercedes-Benz eCitaro Fuel Cell City Bus
https://fuelcellsworks.com/news/mercede ... ting-2022/
MSC Cruises to Bring World-First LNG-Operated #fuelcell on Board MSC Europa
https://fuelcellsworks.com/news/msc-cru ... sc-europa/
https://fuelcellsworks.com/news/chinese ... d-engines/
https://fuelcellsworks.com/news/mobilit ... the-start/

So FuelCells for trucks is quite a practical idea, I don't know why Nikola wants to make fancy battery claims on top.

I can't believe the scams out there though, I saw this "Waterseer" titled video on youtube many times but it looked boring so I never watched it, but then YouTube autoplay/next-video played it, it's hilarious and fascinating how cheeky the scammers are out there.
It was all the people who paid money on IndieGoGo Crowdfund asking where is their water machine that really is the kicker.
Speed Kills Range, 10mph = 46 miles range, 20mph = 20 miles, 30mph = 8 miles rangehttps://goo.gl/1JNL53
Over Charging Kills ur battery bit.ly/1hzWKl4
Consider PAS as your only throttle https://goo.gl/Kg1F8F
Fuel-Cell is the ultimate battery coupled with 4th-gen Nuclear
https://goo.gl/TcKtHs https://goo.gl/ZhFFot https://goo.gl/gfa215
10 Square Miles of solar panels = 0.12GW average power! https://goo.gl/Ub1S39

User avatar
TheBeastie   1 MW

1 MW
Posts: 1993
Joined: Jul 28 2012 12:31am
Location: Melbourne Australia

Re: Thread for new battery breakthrough PR releases

Post by TheBeastie » Nov 21 2019 8:12am

When you see some "new amazing" battery tech company get swallowed by Tesla or some other automaker for $50million you have to be a bit dubious that the tech was anything special.. If it could double lithium cell performance the tech would be worth billions.

But today I saw a headline worthy of this thread simply because of the raw size of the money changing hands...
BMW places $11 billion order for battery cells
https://europe.autonews.com/automakers/ ... tery-cells

Battery cells for all!
Image
Speed Kills Range, 10mph = 46 miles range, 20mph = 20 miles, 30mph = 8 miles rangehttps://goo.gl/1JNL53
Over Charging Kills ur battery bit.ly/1hzWKl4
Consider PAS as your only throttle https://goo.gl/Kg1F8F
Fuel-Cell is the ultimate battery coupled with 4th-gen Nuclear
https://goo.gl/TcKtHs https://goo.gl/ZhFFot https://goo.gl/gfa215
10 Square Miles of solar panels = 0.12GW average power! https://goo.gl/Ub1S39

furcifer   10 kW

10 kW
Posts: 617
Joined: Dec 21 2018 12:36pm

Re: Thread for new battery breakthrough PR releases

Post by furcifer » Nov 23 2019 5:13pm

Honk wrote:
Nov 20 2019 5:32am
Any technical oddity in press releases if often a sign of bullshit and wapor ware.
The press release itself is just a fraud and the intent is raising investment capital.
It's not a press release it's an article on the paper published in Advanced Materials: https://onlinelibrary.wiley.com/doi/abs ... .201902518

Numerous sites have published the article
https://www.google.com/search?sxsrf=ACY ... 9JhgUNI8sA

I'm not sure how legitimate the Advance Materials journal is but it's been around for 30 years. The paper itself is from the University of Illinois. I don't see any investment opportunities being presented.

As for the charge/recharge cycles reference it doesn't seem all that unusual. From what I've read it's a more specific reference than "discharge cycles"; "discharge cycles" seems to refer to a 100% to 0% range while charge/recharge cycles seems to refer to a narrower more usable range.

I wouldn't classify this as fraud, it seems much more inline with the "wishful thinking" that typically follows these types of journal articles. Somewhere in the fine print the practical use of such technology is prohibitive for some reason or the current state of development means even if it does pan out it could be decades before it come to market, if at all. In the interim something else could come along and this technology gets shelved.

User avatar
Honk   100 W

100 W
Posts: 226
Joined: Oct 10 2011 3:31pm

Re: Thread for new battery breakthrough PR releases

Post by Honk » Dec 01 2019 11:17am

Ok, I change my statement to "Any strange technical oddities in a press release, articles with extraordinary claims or technical papers is often a fraudulent sign".
Efficiency is king!

User avatar
emmgee   10 W

10 W
Posts: 80
Joined: Jun 16 2010 6:34am
Location: CH

Re: Thread for new battery breakthrough PR releases

Post by emmgee » Dec 06 2019 6:15am

Interesting paper... looks scientifically sound and the authors from UIC, Argonne and Purdue are credible.
Swagelock cells have been built and tested based on theoretical calculations of the novel ingredients (Li as anode, CO2 as cathode with MoS2 as catalyst and a ionic liquid/dimethyl sulfoxide electrolyte with a (still) F containing Li-salt). Voltage around 2.9V with a high overvoltage needed for charging (at around 4.5V).
My impression: Far from being ready for the mass market in a short time, but a precious contribution to the battery world and an interesting potential on a longer time scale.
Modified Scott Nitrous, 74V, MagicPieV2, waiting for Lebowski-Controller.
eScooter vRone, waiting for Lebowski-Controller and brushless motor.

Hillhater   100 GW

100 GW
Posts: 10808
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Thread for new battery breakthrough PR releasesa

Post by Hillhater » Dec 19 2019 7:52am

IBM claim to have the next big deal in batteries..
https://www.techrepublic.com/article/ib ... 2449370598
According to IBM, tests of the new battery "proved it can be optimized to surpass the capabilities of lithium-ion batteries in a number of individual categories including lower costs, faster charging time, higher power and energy density, strong energy efficiency and low flammability."

That faster charging time IBM mentioned is one of the standouts of its report on this battery breakthrough: It can reportedly reach an 80% charge in just five minutes, all without compromising discharge capacity.

Along with that impressive recharge rate are several other performance improvements, IBM said:

It can reach a power density of more than 10,000 watts per liter;
It can reach an energy density of more than 800 watt hours per liter, which is comparable to modern lithium ion batteries;
It has an energy efficiency (defined by IBM as "the ratio of the energy to discharge the battery over the energy to charge the battery") of over 90%.
This forum owes its existence to Justin of ebikes.ca

User avatar
Toorbough ULL-Zeveigh   100 MW

100 MW
Posts: 2598
Joined: Feb 09 2007 3:02am
Location: Marlboro

world's tiniest gingerbread house

Post by Toorbough ULL-Zeveigh » Dec 19 2019 3:13pm

researcher's goofin' off is why it's taking so long for a new battery breakthrough.
made his house of silicon while he made the snowman of particles that are used in lithium-ion battery research, including nickel, cobalt and aluminum.

https://www.cbc.ca/news/canada/hamilton ... -1.5401274

User avatar
MitchJi   1 GW

1 GW
Posts: 3181
Joined: Jun 02 2008 8:09pm
Location: Marin County California

Re: Thread for new battery breakthrough PR releases

Post by MitchJi » Dec 20 2019 12:53pm

Seems promising:
https://cleantechnica.com/2019/12/18/ib ... e-battery/
IBM Changes The Energy Storage Game With Cobalt-Free Battery
Best Wishes!

Mitch


The best quality batteries and lowest priced batteries for DIY EV's are tier 1 OEM Quality Cells from salvaged (wrecked) EV packs. Three examples are Chevy Volt and Nissan Leaf and Tesla Model 3 packs.

Nissan Leaf Module specs are here
Chevy Volt Pack Info - Salvage 16kwh Packs Under $2k here

User avatar
A-DamW   1 µW

1 µW
Posts: 1
Joined: Dec 19 2019 12:43pm

Re: Thread for new battery breakthrough PR releases

Post by A-DamW » Jan 11 2020 5:23pm

Hey first time poster, LONG time lurker (~2009).

Did some searching of this thread, did not see this PR about Tesla corp. battery research, so here it is:

https://pv-magazine-usa.com/2019/09/09/ ... n-battery/

Jeff Dahn, Tesla’s main battery research partner, seems to have a substantial background in real-world battery tech-to-market.

Do a search for: "tesla 20 year batteries" and "Jeff Dahn" for more info.

User avatar
fechter   100 GW

100 GW
Posts: 14714
Joined: Dec 31 2006 3:23pm
Location: California Bay Area, USA

Re: Thread for new battery breakthrough PR releases

Post by fechter » Jan 12 2020 1:18pm

Some advances in lithium-sulfur batteries. LiS has the potential for twice the energy density of present batteries and lower cost.

The problem has been a large amount of expansion of the sulfur part during discharge, which breaks up the electrode structure. The new approach is to cover nano particles of sulfur with a 'shell' material then dissolve away part of the sulfur inside so there is room for expansion without cracking the shell.

https://arstechnica.com/science/2020/01 ... ur-future/
"One test is worth a thousand opinions"

User avatar
Honk   100 W

100 W
Posts: 226
Joined: Oct 10 2011 3:31pm

Re: Thread for new battery breakthrough PR releases

Post by Honk » Jan 16 2020 2:19pm

Loosing 25% capacity after 200 cycles is not impressive, rather lousy actually.
But they don't seem to care about that small "issue".
Easily fixed they might think, but probably not and the waiting for truly good LiS batteries continues....
Efficiency is king!

hypertoric_amplituhedron   100 W

100 W
Posts: 214
Joined: Dec 02 2016 7:57pm
Location: Land of the Florida Man

Re: Thread for new battery breakthrough PR releases

Post by hypertoric_amplituhedron » Jan 20 2020 8:58pm

New little breakthrough in preventing oxygen release from reacting with electrolytes, involving a molten salt treatment to the Li-rich cathode.

https://techxplore.com/news/2020-01-gra ... icles.html
There are two types of people in this world.

1. Those who can extrapolate from missing information.

hypertoric_amplituhedron   100 W

100 W
Posts: 214
Joined: Dec 02 2016 7:57pm
Location: Land of the Florida Man

Re: Thread for new battery breakthrough PR releases

Post by hypertoric_amplituhedron » Jan 22 2020 10:20pm

New anode tech: coat a porous silicon anode in alumina, then let the alumina saturate with lithium. It becomes a protective catalyst layer for the cathode, and keeps max capacity stable over 100's of cycles. So, not only do we get a decent jump in capacity, but cycle life as well.

https://phys.org/news/2020-01-cells-sil ... tings.html

Image
There are two types of people in this world.

1. Those who can extrapolate from missing information.

maydaverave   10 kW

10 kW
Posts: 541
Joined: Jan 13 2009 11:14pm

Re: Thread for new battery breakthrough PR releases

Post by maydaverave » Mar 10 2020 8:38pm

"To overcome those effects, Samsung’s researchers proposed utilizing, for the first time, a silver-carbon (Ag-C) composite layer as the anode. The team found that incorporating an Ag-C layer into a prototype pouch cell enabled the battery to support a larger capacity, a longer cycle life, and enhanced its overall safety. Measuring just 5µm (micrometers) thick, the ultrathin Ag-C nanocomposite layer allowed the team to reduce anode thickness and increase energy density up to 900Wh/L. It also enabled them to make their prototype approximately 50 percent smaller by volume than a conventional lithium-ion battery."


https://news.samsung.com/global/samsung ... ure-energy
e-bikekit 50v 9.2ah cellman pack

User avatar
neptronix   100 GW

100 GW
Posts: 14179
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: Thread for new battery breakthrough PR releases

Post by neptronix » Mar 11 2020 9:54am

Hot off the presses..
John Goodenough, inventor of the original lithium battery, has a buyer and a plan to commercialize his glass based batteries..

https://www.theregister.co.uk/2020/03/0 ... s_battery/

The test cell had almost the capacity of an 18650 but was the size of a coin cell and can produce 20,000+ cycles.
We're talking about >1000whrs/kg here which would make all the other solid state technologies being developed totally irrelevant :shock:
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

Hillhater   100 GW

100 GW
Posts: 10808
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Thread for new battery breakthrough PR releases

Post by Hillhater » Mar 11 2020 9:55pm

Timing often dictates who wins commercially, ..IE, who gets their product to consumers first has a huge advantage even if the technology is not the “best” ......
And..
Goodenough reckons that solid-state batteries could become commercially successful within the next five to 10 years.
Some of us (And JB G himself ?) ..may not be around long enough to benefit from these developments.
This forum owes its existence to Justin of ebikes.ca

User avatar
Honk   100 W

100 W
Posts: 226
Joined: Oct 10 2011 3:31pm

Re: Thread for new battery breakthrough PR releases

Post by Honk » Mar 12 2020 3:58am

Hillhater wrote:
Mar 11 2020 9:55pm
Some of us (And JB G himself ?) ..may not be around long enough to benefit from these developments.
Unless life extension research is successful within the next 5-10 years... :mrgreen:
Efficiency is king!

memy   1 W

1 W
Posts: 52
Joined: Feb 01 2008 5:26am
Location: Australia mitcham

Re: Thread for new battery breakthrough PR releases

Post by memy » May 20 2020 12:28am

NCMA
A new break through every week I know
https://www.greencarcongress.com/2019/0 ... svolt.html
BUT now SVOLT are claiming they will be shipping next year https://insideevs.com/news/424185/svolt ... n-battery/
I assume the insideevs is getting their content from https://www.youtube.com/watch?v=Amnu5FBL58g jump to 26.45 onwards, rather long winded. (Subtitles)

Hillhater   100 GW

100 GW
Posts: 10808
Joined: Aug 03 2010 10:33pm
Location: Sydney ..(Hilly part !) .. Australia/ Down under !

Re: Thread for new battery breakthrough PR releases

Post by Hillhater » May 20 2020 8:50pm

Is there actually a set date for Tesla’s “ Battery Day”. ?
This forum owes its existence to Justin of ebikes.ca

memy   1 W

1 W
Posts: 52
Joined: Feb 01 2008 5:26am
Location: Australia mitcham

Re: Thread for new battery breakthrough PR releases

Post by memy » May 21 2020 12:44am

No.
Now in two parts, sometime next month video and then bums on seat at some point. He really likes an audience :)

Post Reply