Re: RC Lipo series charging tutorial

Post by soaresdacosta » Dec 24 2013 12:45pm

Hi guys,

Just one question related to this. Im going to build a 24s 2p made of 8 6s5000mha batteries. First i put 2 packs permanent in parallel, including the balance leads, then i series the 4 groups. To charge I disconnect the series plug and charge 6s2p individual. So the question is, wen i connect my charger, he ask if i have batteries in parallel. Well, i have a 6s10mha made of 2 batteries. So...i have batteries in parellel or not ?



Take care guys
Luis.

User avatar
izeman   10 GW

10 GW
Posts: 4989
Joined: Jun 21 2011 8:25am
Location: vienna, austria
Contact:

Re: AW: RC Lipo series charging tutorial

Post by izeman » Dec 24 2013 4:58pm

First of all: yes. You got it right.
Second: two batteries parallel are like one bigger one. Absolutely no difference, neither from the motor side, nor from the charger side.
What charger do you have? I've never heard of a charger along me if a battery is in parallel...

assaf   1 mW

1 mW
Posts: 16
Joined: Mar 21 2013 3:46pm
Location: Israel

Re: RC Lipo series charging tutorial

Post by assaf » Dec 24 2013 5:02pm

The charger wants to know if the batteries are paralleled (and how many) to multiply the amount of current by that number (my powerlab 6 does that). For example, if you set it to charge at 3A 2P, it'll actually output 6A.
Specialized demo 8 + crystalyte H4040: http://crystalyteondemo.blogspot.com

User avatar
soaresdacosta   1 kW

1 kW
Posts: 461
Joined: Jan 26 2011 12:08pm
Location: Portugal / Europe

Re: RC Lipo series charging tutorial

Post by soaresdacosta » Dec 25 2013 4:53pm

Hi guys,

assaf thats my charger...powerllab 6. Other than the amount of amps put by the charger, no big deal , if they are in parallel or not ? Right ?

Thanks,
Luis.

assaf   1 mW

1 mW
Posts: 16
Joined: Mar 21 2013 3:46pm
Location: Israel

Re: RC Lipo series charging tutorial

Post by assaf » Dec 25 2013 5:08pm

You can parallel 2 batteries (in your case amounting to 6s 10Ah) or 10, the charger doesn't care as long as your pack is 6s or less.
What you generally don't want is to push passed 1C of amps, which is 5A for 1 battery, 10A for 2, 15A for 3, etc.
Setting the PowerLab to give 5A 2P is equal to 10A 1P.
Hope this helps.
Specialized demo 8 + crystalyte H4040: http://crystalyteondemo.blogspot.com

User avatar
soaresdacosta   1 kW

1 kW
Posts: 461
Joined: Jan 26 2011 12:08pm
Location: Portugal / Europe

Re: RC Lipo series charging tutorial

Post by soaresdacosta » Dec 25 2013 5:19pm

Yes, it helps. Now I understand, wy the charger ask, how many batteries i have in parallel .

Take care,
Luis.

User avatar
amberwolf   100 GW

100 GW
Posts: 28584
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: RC Lipo series charging tutorial

Post by amberwolf » Jan 02 2014 10:49am

izeman wrote:nope. any RC balance charger NEEDS the balance plug do be connected to charge. otherwise it will refuse to charge a lipo chemistry.
I wish that was true, but at least for the Turnigy Accucell6 (and any other "clone" of it, or whatever it is a clone of) doesn't--it will cheerfully charge a pack wihtout the balance connector attached at all, with just the main + - leads hooked up. Doesn't give you any alert about it either, that requires a bypass--it just starts charging as normal, in either LiPo or LiIo mode, for Charge or Fast Charge. I haven't checked to see if it will do it in Balance Charge mode--I've always had the balance plug hooked up for that one.

User avatar
neptronix   100 GW

100 GW
Posts: 14138
Joined: Jun 15 2010 5:56pm
Location: California refugee living in Utah, USA
Contact:

Re: RC Lipo series charging tutorial

Post by neptronix » Jan 02 2014 2:39pm

My voodoo spell to get my icharger and hyperion chargers doing bulk charges for 3 years isn't too hard to cast; you will find the instructions on how to cast the spell in the owner's manual of both of these chargers, or by poking around in the menus.

;)
"Love and compassion are necessities, not luxuries. Without them, humanity cannot survive." - Dalai Lama

My first major build: 1.6kW 8T MAC motor on a Trek 4500.
The new all-arounder: Leafmotor 1500w @ 4kW on a Turner O2 full suspension.
The monster scooter: 20" eZee on a Cannondale Semi Recumbent.
Whipper-snapper: ? on a lightweight BikeE Semi Recumbent

drew12345   10 kW

10 kW
Posts: 899
Joined: Oct 16 2013 8:34pm
Location: MD, USA

Re: RC Lipo series charging tutorial

Post by drew12345 » Feb 24 2014 8:16am

neptronix wrote:My voodoo spell to get my icharger and hyperion chargers doing bulk charges for 3 years isn't too hard to cast; you will find the instructions on how to cast the spell in the owner's manual of both of these chargers, or by poking around in the menus.

;)
Hey Neptronix. I want to bulk charge 12s. I went to the charge mode in my iCharger 3010b. I see where I can set to Lipo 4.1 and set the amps. However, the voltage only goes up to 37v 10s. Am I missing something here?

User avatar
Ykick   100 GW

100 GW
Posts: 5558
Joined: Nov 26 2009 6:10pm
Location: San Diego, California

Re: RC Lipo series charging tutorial

Post by Ykick » Feb 24 2014 8:25am

drew12345 wrote:
Hey Neptronix. I want to bulk charge 12s. I went to the charge mode in my iCharger 3010b. I see where I can set to Lipo 4.1 and set the amps. However, the voltage only goes up to 37v 10s. Am I missing something here?
As generic reply:

iCharger 3010b is designed to charge up to 10S. Some people run 10S so it may be used for bulk charging up to that cell count - pack voltage. 12S ain't gonna happen with a 3010b unless you break it down to smaller series strings.
Talent must not be wasted.... Those who have talent must hug it, embrace it, nurture it and share it lest it be taken away from you as fast as it was loaned to you.

- Frank Sinatra

drew12345   10 kW

10 kW
Posts: 899
Joined: Oct 16 2013 8:34pm
Location: MD, USA

Re: RC Lipo series charging tutorial

Post by drew12345 » Feb 24 2014 8:31am

okay, thanks for answer. Makes sense. Just didn't know if there was a way to override the voltage limit.

tomtom123   100 W

100 W
Posts: 284
Joined: Aug 15 2013 9:37pm
Location: New York City, New York

Re: RC Lipo series charging tutorial

Post by tomtom123 » Mar 09 2014 9:40pm

So i want to take 4 packs of these and connect them in series to make packs of 59.2v and 5ah. so 3 packs of 4 lipos in series.
http://www.hobbyking.com/hobbyking/stor ... _pack.html

How would i go about then connect those 3 packs of 59.2v 5ah batteries in parallel to make a 59.2v 15ah battery? What wires do i need to do this?

User avatar
kris   1 mW

1 mW
Posts: 13
Joined: Apr 11 2014 7:08am
Location: Takaka New Zealand

Re: RC Lipo series charging tutorial

Post by kris » Apr 11 2014 6:29pm

Hi I have just brough a 60 v motor what batterys are best to buy please

User avatar
kris   1 mW

1 mW
Posts: 13
Joined: Apr 11 2014 7:08am
Location: Takaka New Zealand

Re: RC Lipo series charging tutorial

Post by kris » Apr 11 2014 7:05pm

Hi can you offer my some advice on what battery's to buy for my 60 volt mid drive motor there are so many options . By the looks of it these rc battery's are the best value in just not sure if i should buy 3 x20 v or 5 x 12 vold will they stay cooler ir there split into 5 also the 5000 2s ?or 3 s ? is throwing me out a bit any suggestions would be awesome thanks please

Thriller   1 W

1 W
Posts: 56
Joined: Mar 16 2014 4:37pm
Location: South East British Columbia Canada

Re: RC Lipo series charging tutorial

Post by Thriller » Apr 28 2014 7:34am

Thanks for the informative post and all the pictures.

User avatar
z50king   100 mW

100 mW
Posts: 43
Joined: Nov 12 2012 5:36am
Location: Upland, CA

Re: RC Lipo series charging tutorial

Post by z50king » Apr 28 2014 11:48pm

you need to run better lead connections. Those stock red ones stink
goped enthusiast

stonezone   100 W

100 W
Posts: 217
Joined: Mar 12 2014 4:25pm
Location: Oahu, Hawaii

Re: RC Lipo series charging tutorial

Post by stonezone » May 01 2014 2:50pm

super quick question and probably a simple answer:

I'm building a 12s4p pack and was going to solder up my own balance harness with a bunch of balance extensions from HK. do I just run them 4 into 1 (pin 1 on each battery balance cable into pin 1 on the balance harness). then there are 4 cells that are being balanced as one and i would occasionally break the pack and individually balance each battery.

When charging (hyperion) I was planning on doing it as one large battery and putting each 4:1 balance harnesses into the balance ports as outlined in this tutorial.

Is there anything else I should be aware of besides the 'golden rules of lipo' ?

TL;DR: making a 4 battery balance adapter is just each pin split into 4, or is there more to it?

Thanks!

SZ
LR-BB on 2014 Glory
Sur-Ron
B B S-HD on some sort of DH Kona frame
2017 GG GP 300 <3

RIP Bobarella

User avatar
oatnet   10 MW

10 MW
Posts: 2340
Joined: Apr 26 2007 3:03pm
Location: SoCal, USA

Re: RC Lipo series charging tutorial

Post by oatnet » May 01 2014 3:51pm

neptronix wrote:Guys, i wrote this 2 years ago but decided to never release it, after watching me and others give people RC Lipo management advice and watch it be ignored and garages get burned down often as a result. RC Lipos make for great batteries if managed properly, but please take *all* of this advice to heart and don't skip over the bits about safety. I do not want to be complicit in encouraging people to play with something that they can't handle.

If you don't think you can handle RC Lipo, don't bother.

The tips provided above have worked for me and many others for many years, but i will NOT assume any liability for what you do with the most powerful and also one of the most dangerous types of batteries you could possibly strap to a bicycle.

-D
Nepo, just found this... nice writeup, and a great contribution to the community. :D

-JD
Member 117 of 26,000+

153v DUNE BUGGY © 164v Vectrix E-Moto © 72v Norco A-line/x5403 © 60v Specialized Enduro Comp/BMC © 72v x5tracycle © 48v TF IO/BMC © 36v Kepler FrictionDrive © Spot-Welding a123 © Pelican Front Packs © Vectrix Battery Replacement © MORE !!


Image大鸡巴 Motors
Knowledge is acquired through experience, everything else is just information - Albert Einstein
"Cheater?" I'm not competing, I'm Commuting!

Tallahau   10 mW

10 mW
Posts: 29
Joined: Jul 17 2014 8:21am

Re: RC Lipo series charging tutorial

Post by Tallahau » Jul 24 2014 7:06am

If I have two brand new 3S 5000mah lipo batteries and I want to series charge them. Should I first charge them up individually and then charge them in series after I discharged them or can I charge them in series right away?

User avatar
Ykick   100 GW

100 GW
Posts: 5558
Joined: Nov 26 2009 6:10pm
Location: San Diego, California

Re: RC Lipo series charging tutorial

Post by Ykick » Jul 24 2014 7:34am

Tallahau wrote:If I have two brand new 3S 5000mah lipo batteries and I want to series charge them. Should I first charge them up individually and then charge them in series after I discharged them or can I charge them in series right away?
I would charge them to same SOC beforehand. Of course, you can always charge via balance leads once the bricks are series wired. All that requires is a simple adapter lead with pins to stick into the appropriate JST cell tap and remember to charge less than 2-3A through the balance wires.
Talent must not be wasted.... Those who have talent must hug it, embrace it, nurture it and share it lest it be taken away from you as fast as it was loaned to you.

- Frank Sinatra

Tallahau   10 mW

10 mW
Posts: 29
Joined: Jul 17 2014 8:21am

Re: RC Lipo series charging tutorial

Post by Tallahau » Jul 24 2014 8:40am

Ykick wrote:
Tallahau wrote:If I have two brand new 3S 5000mah lipo batteries and I want to series charge them. Should I first charge them up individually and then charge them in series after I discharged them or can I charge them in series right away?
I would charge them to same SOC beforehand. Of course, you can always charge via balance leads once the bricks are series wired. All that requires is a simple adapter lead with pins to stick into the appropriate JST cell tap and remember to charge less than 2-3A through the balance wires.
Are the balance wires the ones connected to the JST plug or the i.e 4mm bullet connector? Got me one of these, suppose that would work with the appropriate charger and 4mm series adaptor?

User avatar
izeman   10 GW

10 GW
Posts: 4989
Joined: Jun 21 2011 8:25am
Location: vienna, austria
Contact:

RC Lipo series charging tutorial

Post by izeman » Jul 24 2014 11:58am

the balance wires are the small wires with the jst-xh connectors. the 4mm bullets are the main discharge wires.
the linked connector will work but i almost guarantee you kff with that. it's critical to know in which female end to plug which one of the male battery balance connectors depending on which battery is in which 'series' place. if you don't take care and do it in the wrong order (50% chance) your connectors will be plasma.

BShady   1 kW

1 kW
Posts: 320
Joined: Dec 01 2013 2:27pm
Location: new york

Re: RC Lipo series charging tutorial

Post by BShady » Oct 12 2014 11:55am

Got a qu.

If I first put 2 - 3s batteries in series and then in Parallel With another 2- 3s batteries (these 3s are also in series) how do I connect the balance ports?

Do I first put them in series and then parallel (like the batteries themselves) or just all in parallel?

Thank you

adrock8519   1 W

1 W
Posts: 51
Joined: Jun 25 2013 7:14am

Re: RC Lipo series charging tutorial

Post by adrock8519 » Oct 12 2014 3:21pm

BShady wrote:Got a qu.

If I first put 2 - 3s batteries in series and then in Parallel With another 2- 3s batteries (these 3s are also in series) how do I connect the balance ports?

Do I first put them in series and then parallel (like the batteries themselves) or just all in parallel?

Thank you

You should parallel your batteries and balacne wires and then join them to the next two paralleled batteries in series. Dont parallel the balance wires between the series packs or it will melt.

stonezone   100 W

100 W
Posts: 217
Joined: Mar 12 2014 4:25pm
Location: Oahu, Hawaii

Re: RC Lipo series charging tutorial

Post by stonezone » Oct 14 2014 4:37pm

Quick question on wiring a 20s4p pack:

what gauge wire should I use:
1) between individual batteries to parallel
2) For the Series connections between Parallel sets
3) from the 20s4p pack to my controller

Also, do most of you directly solder your parallel pack or use plugs between each? Plugs increase the flexibility and everything in the long run, but you can keep things so much cleaner by directly soldering them. In my current 12s6p pack I only use connectors for the Series connections.

thanks,

SZ
LR-BB on 2014 Glory
Sur-Ron
B B S-HD on some sort of DH Kona frame
2017 GG GP 300 <3

RIP Bobarella

Post Reply