Post by silicium » Jan 14 2008 4:32pm

The power unit is à power switching 48V/400W
(objet n°180206228957 on ebay)
Three résistor 0,2 Ohm /50W in serial is connected for limited start current at 8..10A (if omitted the protection power switching start)
few error is detected on schematic... New schematic is ready and new board is ready (my board is a prototype...)
a Mosfet for protect Pack is add and current is cut automaticly if voltage one cell less 2.3V.
The cost of BMS is approx 100 $ (175 $ with supply power)
No kit for sale... Do it yourself !
RH205, A123 4P12S with BMS http://vae-tech.forumactif.org/t8-un-bms-home-made (in french)

User avatar
Snickers   10 mW

10 mW
Posts: 21
Joined: Nov 22 2007 2:45pm

Re: The care and feeding of a123-based packs...

Post by Snickers » Jan 21 2008 10:32am

I work in parallele with Silicium in order to built the full version with 15 cells for a "small" 15S2P battery. :mrgreen:
90% of the job is allready done…
The 15 cells BMS is allready finished, there is some small change in order to accept 56-60V at input in comparison of 12 cells version of silicium
BMS.JPG
BMS.JPG (43.44 KiB) Viewed 3749 times
The 15S2P battery is also rebuilt but still not plug. I must veryfing all links before plug it to BMS.
I have passed a lot of hours to assemble everything. There is something arround 450 components on the board…
And also some couple of hours to verify and test everything !
I hope now, they will be no burning when I will plug the battery ! :roll:
bat.JPG
bat.JPG (27.85 KiB) Viewed 3749 times

Randomly   100 W

100 W
Posts: 100
Joined: Jan 24 2008 6:53am

Re:

Post by Randomly » Jan 24 2008 7:21am

silicium wrote:I do not know if I put my message in the right place...
I make a BMS for a battery A123 (4P12S)...
What do you think of my circuit? (BMS A123 x12 eng.pdf)
Best regards,
Silicium
I'm kind of late finding this thread but I noticed looking at Silicium's schematic that there is a potential problem with the way FINCHARGE is used to shut off Q16, TIP 142.
The input offset voltage of the LM358 can be up to 7mv so even though you've pulled the + input of the LM358 to ground it's possible Q16 will still be flowing up to 70mA of current to the battery stack. You may have already found and addressed this problem, but I bring it up in case you haven't. You may want to find a different way to shut Q16 off.
One other minor point is that for a full 15 cell stack and charging voltages in excess of 50V you have potentials in excess of the voltage rating of the BUZ11. This may not be an issue though since under normal operating conditions the BUZ11 will see the charging voltage - the battery stack voltage.
It's a nice design and a very well laid out schematic. Hope my comments are helpful.

User avatar
silicium   10 W

10 W
Posts: 67
Joined: Nov 12 2007 2:38pm
Location: Albi, France
Contact:

Re: The care and feeding of a123-based packs...

Post by silicium » Jan 24 2008 11:20am

Thanks for the feedback !
Schematic is updated... and work fine (tested on 2 board)
for current limit off: Rshunt up to 1 Ohms (current off is <1mA)
all mosfet are RFP70N06 or RFP60N06 Q100 is IRFB4110 (100V, 4.5mOhms)

in sub-circuit for control cell, news components is added for protected ... In prototype, TCM809 is dead...
BMS A123 x15V5complet.pdf
Schematic V5
(87.6 KiB) Downloaded 682 times
BMS A123 Cell.pdf
Schematic sub-circuit for Cell 1..15 V5
(26.1 KiB) Downloaded 531 times
Attachments
color board.pdf
new board (all modifications)
(105.77 KiB) Downloaded 386 times
RH205, A123 4P12S with BMS http://vae-tech.forumactif.org/t8-un-bms-home-made (in french)

Randomly   100 W

100 W
Posts: 100
Joined: Jan 24 2008 6:53am

Re: The care and feeding of a123-based packs...

Post by Randomly » Jan 24 2008 12:15pm

silicium wrote:Thanks for the feedback !
Schematic is updated... and work fine (tested on 2 board)
for current limit off: Rshunt up to 1 Ohms (current off is <1mA)
all mosfet are RFP70N06 or RFP60N06 Q100 is IRFB4110 (100V, 4.5mOhms)

in sub-circuit for control cell, news components is added for protected ... In prototype, TCM809 is dead...
BMS A123 x15V5complet.pdf
BMS A123 Cell.pdf
I can see my original comments where a bit out of date, you've gone through a number of revisions since the first schematic I saw. Very nice work. Looks great ;-)
A couple thoughts I had, You shut off Q3 when the safety signal is out of range, but you don't seem to shut off Q1. or did I miss something?

On the CELL1 schematic couldn't you connect R20 and R22 to the collector of Q6 and get rid of Q7? or is the gain at Q6 too low and the transition on Q6 too soft?

User avatar
Snickers   10 mW

10 mW
Posts: 21
Joined: Nov 22 2007 2:45pm

Re: The care and feeding of a123-based packs...

Post by Snickers » Jan 24 2008 1:55pm

After several cycles, I still have nothing burned...and it's work perfectly.
I have calibrate balancing at 100mA for my small batterie.
A picture with Balancing in progress.
P1070086_red_2.jpg
P1070086_red_2.jpg (52.16 KiB) Viewed 3404 times
I use only for the moment 60v mosfet.
Maximal battery voltage is 54V and charger output is 57V maximal.
Batterie capacity was checked two time. Nominal cells voltage seems to be 3,2V and not 3,3V
Discharging curve at ~5,6A:
décharge_5,6A.GIF
décharge_5,6A.GIF (9.46 KiB) Viewed 6074 times
I must focus now on a box
Last edited by Snickers on Feb 06 2008 8:08am, edited 1 time in total.

User avatar
silicium   10 W

10 W
Posts: 67
Joined: Nov 12 2007 2:38pm
Location: Albi, France
Contact:

Re: The care and feeding of a123-based packs...

Post by silicium » Jan 24 2008 2:30pm

Randomly wrote: On the CELL1 schematic couldn't you connect R20 and R22 to the collector of Q6 and get rid of Q7? or is the gain at Q6 too low and the transition on Q6 too soft?
No, Q6 is work must too linearly... The schematic is surely simplifiable ! but it work fine...
RH205, A123 4P12S with BMS http://vae-tech.forumactif.org/t8-un-bms-home-made (in french)

User avatar
flip_normal   100 W

100 W
Posts: 258
Joined: Jul 12 2007 10:30pm
Location: london

Re: The care and feeding of a123-based packs...

Post by flip_normal » Jan 28 2008 5:09pm

Hi Silicium/Snickers,

well impressive BMS/charger, very nice work. 8)

What are the final specs for this? How many watts does it output? How long does it take to charge your packs?

How hard would it be to significantly increase the output power of this design?

So what's next? Any chance of a open design programmable controller? :twisted: :roll:

User avatar
Snickers   10 mW

10 mW
Posts: 21
Joined: Nov 22 2007 2:45pm

Re: The care and feeding of a123-based packs...

Post by Snickers » Jan 31 2008 9:27am

I have plan to charge my 15S2P with less than half a hour with very simple power supply 56V 10A. Today, I use 56V 2,5A with three small adapter in series.

Output power from battery is not limited…for my 15S2P, 100A if you want.You must only add few mosfet in parallel for the battery cutoff when BMS detected one element empty.

My battery link are design to support continuous 50A. The cutoff mosfet 3,5 milliohms 60V extract from one Dewalt BMS will support à continuous 30A with a small heat dissipater. These mosfet from Dewalt BMS are really excellent for this job.

Protection again short cut is performed with a external 30A fuse, a 20A re-armable fuse and the internal battery fuse link already inside Delwalt pack. This is in order to be safe with a battery pack able to deliver 10KW instant power!

100mA balancing takes around 5 minutes at the end of charge. 500mA balancing are possible by added some small copper heat dissipater near balancing transistor. Perhaps I will do if I upgrade my battery to 15S4P version.

About an open design programmable controller, I think Silicium don't have planned to do this. Aim was to propose an affordable design for everybody. There is clearly really more components than one with CPU, but no programming tools are necessary to built it.

rf   1 kW

1 kW
Posts: 381
Joined: Sep 18 2007 8:02pm

Re: The care and feeding of a123-based packs...

Post by rf » Jan 31 2008 11:26am

Snickers wrote:...

About an open design programmable controller, I think Silicium don't have planned to do this. Aim was to propose an affordable design for everybody. There is clearly really more components than one with CPU, but no programming tools are necessary to built it. ...
There are good microcontrollers available that only require a USB cable and a PC to program them. The development software is free. A complete development board can be had for $15.

http://moderndevice.com/index.shtml

User avatar
silicium   10 W

10 W
Posts: 67
Joined: Nov 12 2007 2:38pm
Location: Albi, France
Contact:

Re: The care and feeding of a123-based packs...

Post by silicium » Feb 01 2008 5:52am

News of my pack 4P12S
Test with 14 Amp discharge:
Image
The pack restores 9.1 Ah representing over 98% of the theoretical capacity :D
Well, given all the previous tests, the opposite would have been surprising ...
Now I check that the charger is 'solid' ... Before finishing the integration into the box. If not for news, I retrieved from the original BMS packs dewalt of Mosfets with a RDSon of 3.5 mOhms ... I put 2 in parallel to cut the battery when the BMS indicates an item is empty. The fall of terminal voltage of mosfet at 14A was ... 20mV The fuse was 30A of 55mV drop him!
The total voltage drop (cablage relay + + + mosfet fuse) was 350mV or an equivalent resistance total 0.35/14 = 25 mohm. A 14A I lost 5W = 14x14x25 in the wiring or 1% of the power in charge
RH205, A123 4P12S with BMS http://vae-tech.forumactif.org/t8-un-bms-home-made (in french)

User avatar
Microbatman   1 kW

1 kW
Posts: 304
Joined: Nov 26 2007 1:13pm
Location: Lantana Texas
Contact:

Re: The care and feeding of a123-based packs...

Post by Microbatman » Feb 05 2008 9:58pm

Nice Work!!!!!!!!!

Love that graph. Super info as I am in the process of putting together a 12cell pack as well. Now I have some data about where to LVC should be.

What type of equipment are you using to put that kind of a continious load on these???
MotorCrystalyte X5304 20 Inch Rear Wheel DISC Brake Controller Crystalyte 48A72V4110MOSFETS
Batteries A123 24s2p
Charger Mastech 5020
Frame Azonic Steelhead
Grateful/fortunate/blessed to have the resources and family support to enjoy my ebike hobby

User avatar
Snickers   10 mW

10 mW
Posts: 21
Joined: Nov 22 2007 2:45pm

Re: The care and feeding of a123-based packs...

Post by Snickers » Feb 06 2008 7:00am

About continous load, I use a resistance extract form hair dryer. It's gave me at 48V 265 watts heating .
The most simple solution is to use 3-4 automotive ligh bulb 12v 50-55 watts in serie.
Silicium use something like this.
My battery (box+BMS only=1,35Kg) + 2,4 Kg battery = Total 3,75 Kg 8,3 Lb
Design of box is for 15S4P + some space inside for circuit bracker,...
P1070106_masse_boite+BMS_red.jpg
P1070106_masse_boite+BMS_red.jpg (32.38 KiB) Viewed 3853 times
I have finished the assembly and I drive now with my 15S2P batterie with BMS from silicium
Batterie_red2.jpg
Batterie_red2.jpg (44.96 KiB) Viewed 3853 times
First test 4,28Ah+ 0,132Ah (consumption from my 48v Led lighting + controler)
P1070109_resumé_red.jpg
P1070109_resumé_red.jpg (27.94 KiB) Viewed 3838 times
Last edited by Snickers on Feb 19 2008 3:22pm, edited 2 times in total.

User avatar
silicium   10 W

10 W
Posts: 67
Joined: Nov 12 2007 2:38pm
Location: Albi, France
Contact:

Re: The care and feeding of a123-based packs...

Post by silicium » Feb 06 2008 3:25pm

picture of my load for discharge at 14A 8)

3x120W (automotive bulb H4) + 3x55W (old automotive bulb)

Image
RH205, A123 4P12S with BMS http://vae-tech.forumactif.org/t8-un-bms-home-made (in french)

User avatar
silicium   10 W

10 W
Posts: 67
Joined: Nov 12 2007 2:38pm
Location: Albi, France
Contact:

Re: The care and feeding of a123-based packs...

Post by silicium » Feb 12 2008 9:37am

It's Ok in my bike :D
speed 33..35 km/h (it's good for me !)
Image
BMS + Pack 4P12S + box

Image
battery fixed in the box

Image
The charger 400W (charge time 1H)
RH205, A123 4P12S with BMS http://vae-tech.forumactif.org/t8-un-bms-home-made (in french)

User avatar
Jozzer   100 kW

100 kW
Posts: 1069
Joined: Apr 19 2007 8:32am
Location: Swindon UK
Contact:

Re: The care and feeding of a123-based packs...

Post by Jozzer » Feb 12 2008 1:37pm

Very nice Silicium, good work :D
Mazda MX-5. 300KW power. Soliton 1 controller, 11" Kostov motor, 20KW/H Turnigy Lipo for 60-100 miles range. 120mph top speed.
Hudson Kindred Spirit 3 wheeler. Twin Agni setup, 300KG 80KW. 100mph top speed (maybe more, but no-one has the guts to try!)
Aprilia RS125, Agni motor, 600A 96v Kelly controller, 6kw/h pack
Dual Agni Ducati.
Countless ebikes and trikes..
http://www.Jozztek.com

User avatar
Frxdy   10 mW

10 mW
Posts: 29
Joined: Jan 07 2008 9:30pm
Location: Orrington, Maine
Contact:

Re: The care and feeding of a123-based packs...

Post by Frxdy » Feb 14 2008 5:22am

For those interested...this auction is about 8 hours old... buy it now, $110. He has two, look for the other auction.

http://cgi.ebay.com/36V-DEWALT-BATTERY- ... dZViewItem

<edit> Sold! This post can be deleted.
Seven days without pizza makes one weak.

User avatar
efreak   100 W

100 W
Posts: 227
Joined: Jul 31 2007 3:48pm
Location: Toronto
Contact:

Re: The care and feeding of a123-based packs...

Post by efreak » Feb 19 2008 3:14pm

that's nice work silicium and the battery compartment as well could retire on that alone you would think :D

i am currently trying to construct a dc dc converter based charger( used as single chargers) hopefully with help from doc and gary welcome your input on that thread as well .

but really nice work and its been coming for a long time now and looks tight.
5304 x-lyte
new72v 35-40
26" supercycle

working on 80 cell m1

User avatar
jeffkay   100 W

100 W
Posts: 115
Joined: Sep 15 2007 1:03am

Re: The care and feeding of a123-based packs...

Post by jeffkay » Mar 14 2008 11:24pm

Wow, That's what I call a WOODY!

User avatar
Microbatman   1 kW

1 kW
Posts: 304
Joined: Nov 26 2007 1:13pm
Location: Lantana Texas
Contact:

AddingTapsFor6CellPAck

Post by Microbatman » Apr 12 2008 2:02pm

*************** Adding Taps to a 6 cell pack *************************************8

Start with a 6 cell brick
I choose to use the hyperion/polyquest type of tap as that seems the most common.
http://home.comcast.net/~truerc/Charge/chargers.htm
It is the 7 pin balance connector from here (bottom of page on right $4)



File too big error will post pics later
Attachments
batteryTap1S.JPG
7 Wire Hyperion/Polyquest Tap
batteryTap1S.JPG (36.22 KiB) Viewed 4760 times
batteryTap2s.JPG
OddWires Go on Top
batteryTap2s.JPG (37.54 KiB) Viewed 4746 times
batteryTap3s.JPG
BlueNumbersAreWhereWiresGo
batteryTap3s.JPG (35.11 KiB) Viewed 4737 times
batteryTap4s.JPG
BlueNumbersShowPositionofWireNumber
batteryTap4s.JPG (37.56 KiB) Viewed 4738 times
batteryTap5s.JPG
EvenWiresGoOnBottom
batteryTap5s.JPG (33.66 KiB) Viewed 4730 times
batteryTap6s.JPG
batteryTap6s.JPG (33.19 KiB) Viewed 4729 times

User avatar
Microbatman   1 kW

1 kW
Posts: 304
Joined: Nov 26 2007 1:13pm
Location: Lantana Texas
Contact:

Wire by Wire Pics

Post by Microbatman » Apr 15 2008 7:50pm

Here it is wire by wire
Attachments
wire1.JPG
wire1.JPG (31.18 KiB) Viewed 4154 times
wire2.JPG
wire2.JPG (30.94 KiB) Viewed 4154 times
wire2a.JPG
wire2a.JPG (27.67 KiB) Viewed 4150 times
wire3.JPG
wire3.JPG (40.24 KiB) Viewed 4144 times
wire3a.JPG
wire3a.JPG (34.09 KiB) Viewed 4141 times
wire4.JPG
wire4.JPG (33.99 KiB) Viewed 4142 times
wire4a.JPG
wire4a.JPG (24.58 KiB) Viewed 4138 times
wire5.JPG
wire5.JPG (33.96 KiB) Viewed 4135 times
wire5a.jpg
wire5a.jpg (28.99 KiB) Viewed 4125 times
wire6.jpg
wire6.jpg (33.29 KiB) Viewed 4126 times
MotorCrystalyte X5304 20 Inch Rear Wheel DISC Brake Controller Crystalyte 48A72V4110MOSFETS
Batteries A123 24s2p
Charger Mastech 5020
Frame Azonic Steelhead
Grateful/fortunate/blessed to have the resources and family support to enjoy my ebike hobby

User avatar
Microbatman   1 kW

1 kW
Posts: 304
Joined: Nov 26 2007 1:13pm
Location: Lantana Texas
Contact:

Wire by Wire Pics

Post by Microbatman » Apr 15 2008 7:53pm

Wire 7
Attachments
wire7.JPG
wire7.JPG (33.46 KiB) Viewed 4119 times

Mathurin   100 kW

100 kW
Posts: 1166
Joined: May 24 2006 2:49pm
Location: Quebec
Contact:

Re: The care and feeding of a123-based packs...

Post by Mathurin » Apr 19 2008 9:22am

So what's wrong with using a lead charger? EG: 10 cells, 36v lead charger, 4.2v/cell. If that's too aggressive an 11 cell battery would get about 3.8v/cell, letting that float a few mins every now & then should balance the pack since they'll quickly drop below 3.6v/cell without the charger.

http://www.slkelectronics.com/DeWalt/index.htm
SLK Electronics wrote:On a 3-cell pack, I forced a 130-millivolt imbalance by charging one cell. This is a HUGE imbalance due to the small change in voltage with discharge (per the graph discussed previously). Charging was done using a LiPoDapter at a 6A charge rate. A higher charge rate was chosen because higher charge rates cause normal LiPo cells to become unbalanced. The charge regimen could also have used an Astro 109 Lithium charger. The pack was discharged at a constant 20A to 2.7V. Each successive cycle decreased the imbalance. After several cycles there was still some imbalance but only a fraction of the original.
You have to know, not fear, that someday you are going to die. Until you know that and embrace that, you are useless. - Tyler Durden, Fight club. Ditch the fake identity you've created for yourself, walk your own way in a society of mindless drones to become real, you are not your social status.

User avatar
jeffkay   100 W

100 W
Posts: 115
Joined: Sep 15 2007 1:03am

Re: The care and feeding of a123-based packs...

Post by jeffkay » Apr 19 2008 1:51pm

I use one all the time for 4s16p no problems and can't go too high for the unbalance problem.

Mathurin   100 kW

100 kW
Posts: 1166
Joined: May 24 2006 2:49pm
Location: Quebec
Contact:

Re: The care and feeding of a123-based packs...

Post by Mathurin » Apr 21 2008 10:53am

So you're charging the cells with a lead charger, slightly overcharging to balence them?

Are you using a bms? Do you need to periodically re-balance the cells? At what voltage do you charge the cells? Does anyone know to what degree cycle life would be compromised with this approach? Somehow I just don't see tens of thin fragile wires surviving very long in a backpack battery, even less a bms board.
You have to know, not fear, that someday you are going to die. Until you know that and embrace that, you are useless. - Tyler Durden, Fight club. Ditch the fake identity you've created for yourself, walk your own way in a society of mindless drones to become real, you are not your social status.

Post Reply