Post by Stu Summer » Jul 11 2019 9:23pm

I see on Craigslist a Luna triangle battery 52v, 28ah, GA. It is unused, bought in 2017, still with wrappings on the plugs. How much capacity will it have lost? They are asking $600 for it ($1000 new). Thanks.
2013 DB Haanjo Commuter with BBSHD and Zzipper fairing
Marin Rift Zone FS with BBSHD
Kysmo "lab" bike with 350w hub motor
Ryan Vanguard recumbent LWB with a 36v Cyclone 350w middrive and a 56v MAC 5t in the front hub.

User avatar
amberwolf   100 GW

100 GW
Posts: 30304
Joined: Aug 17 2009 6:43am
Location: Phoenix, AZ, USA, Earth, Sol, Local Bubble, Orion Arm, Milky Way, Local Group
Contact:

Re: New 52v battery sat unused for two years...

Post by amberwolf » Jul 11 2019 10:28pm

if they haven't kept it charged the bms probably drained it dead and destroyed it.

flat tire   1 MW

1 MW
Posts: 1968
Joined: Feb 26 2014 12:20am

Re: New 52v battery sat unused for two years...

Post by flat tire » Jul 11 2019 10:39pm

There are lots of GOOD battery options out there, I wouldn't touch that.

User avatar
Drunkskunk   100 GW

100 GW
Posts: 7233
Joined: Apr 14 2007 11:37am
Location: Dallas, Texas. U.S.A.

Re: New 52v battery sat unused for two years...

Post by Drunkskunk » Jul 12 2019 1:14am

If it sat in the heat of a garage, it might have been baked to death. Lithium degrades in the heat.
I would avoid. Batteries have a limited shelf life anyway.
Buy the ticket, take the ride.
Monster Bike:http://endless-sphere.com/forums/viewto ... =6&t=38667

LeftieBiker   10 kW

10 kW
Posts: 712
Joined: Nov 06 2012 1:33am
Location: Upstate NY, United States

Re: New 52v battery sat unused for two years...

Post by LeftieBiker » Jul 12 2019 1:22am

The only way that battery could possibly be ok would be if the BMS was disconnected at the factory and had to be connected by the purchaser. Ping Packs came that way.

john61ct   100 GW

100 GW
Posts: 5412
Joined: Dec 18 2018 2:06pm

Re: New 52v battery sat unused for two years...

Post by john61ct » Jul 12 2019 1:26am

Might be worth testing, if V over 2.5V offer $100

Stu Summer   100 W

100 W
Posts: 100
Joined: Apr 27 2016 8:01pm
Location: Hillsdale, NY

Re: New 52v battery sat unused for two years...

Post by Stu Summer » Jul 12 2019 2:28pm

Thanks everyone! Very clear.
2013 DB Haanjo Commuter with BBSHD and Zzipper fairing
Marin Rift Zone FS with BBSHD
Kysmo "lab" bike with 350w hub motor
Ryan Vanguard recumbent LWB with a 36v Cyclone 350w middrive and a 56v MAC 5t in the front hub.

User avatar
Matador   10 kW

10 kW
Posts: 913
Joined: Jun 29 2016 10:00pm

Re: New 52v battery sat unused for two years...

Post by Matador » Jul 13 2019 8:27am

Could be perfectly Okay... A 28Ah battery is massive and can take a decade to drain from BMS if the pack was stored full...
But if it was stored near 0%, then some of the cells could be toast.

Assuming the cells were NMC, never used, and stored at 50% and a in a garage at ambient temperature of 25°C, the cell should have a remaining usable capacity of above 95% and a DCIR no more than 110% that of brand new. But that's before considering BMS parasitic current draw.... Wich is typically in the uA (microamps) range...

If overall the battery still sits at a voltage anything higher than 50V, i would buy it for a best offer of 400$. 300$ would be more reasonable. Then I would manually balance each cell string as the BMS drain is normally uneven, ofter targeting the first 3 parralleled cell groups...

But if I assume the BMS has a 50uA drain and the guy did not lie about the 2 years duration, then

50 uA = 0.05 mA = 0.00005 A (of BMS draw)
So in 1 hour, thats 0.00005 Ah drained out of 28Ah
So in 1 day, thats 0.0012 Ah
So in 1 year, thats 0.436 Ah
So in Two years, thats about 0.9Ah ...

So in 2 years, such BMS would drain 0.9Ah out of 28Ah. Meaning in two years it would drain about 3.5% of the capacity of that huge battery.....

So unless it was stored empty from the start, I'm quite confident the battery cells are still good.... But look up the specs of the BMS in that pack to be sure about the current it draws... Also, make sure the pack is made of good, brand name 18650 cells... Finally check to see how many cycles (from story, i would assume zero cycles) the pack has.... Also was it stored at 25 or 40 degree celcius ????

Matador
Last edited by Matador on Jul 13 2019 3:47pm, edited 1 time in total.

User avatar
Matador   10 kW

10 kW
Posts: 913
Joined: Jun 29 2016 10:00pm

Re: New 52v battery sat unused for two years...

Post by Matador » Jul 13 2019 8:32am

Another name for this BMs spec figure is "BMS Quiescent current draw"... This figure should be on any respectable BMS datasheet.

Matador

Volt_Ampere   10 W

10 W
Posts: 77
Joined: Apr 18 2018 6:24pm

Re: New 52v battery sat unused for two years...

Post by Volt_Ampere » Jul 13 2019 10:44am

Me - I would not risk it. It might be ok but no way would I pay $600 for it.

LeftieBiker   10 kW

10 kW
Posts: 712
Joined: Nov 06 2012 1:33am
Location: Upstate NY, United States

Re: New 52v battery sat unused for two years...

Post by LeftieBiker » Jul 14 2019 12:12am

But if I assume the BMS has a 50uA drain and the guy did not lie about the 2 years duration, then

50 uA = 0.05 mA = 0.00005 A (of BMS draw)
So in 1 hour, thats 0.00005 Ah drained out of 28Ah
So in 1 day, thats 0.0012 Ah
So in 1 year, thats 0.436 Ah
So in Two years, thats about 0.9Ah ...

So in 2 years, such BMS would drain 0.9Ah out of 28Ah. Meaning in two years it would drain about 3.5% of the capacity of that huge battery.....
Nice BMS if you can get it! They do have a habit of drawing more than that, though - a lot more. I have two 20AH Ping packs. The earlier, hand-built by Ping himself, pack does have a very low vampire drain. The later one, though, draws about 10X that much, by my estimate. It's better to assume the worst but hope for the best than the other way around...

john61ct   100 GW

100 GW
Posts: 5412
Joined: Dec 18 2018 2:06pm

Re: New 52v battery sat unused for two years...

Post by john61ct » Jul 14 2019 9:35am

This is why I would only buy packs where the BMS can easily be disconnected, bypassed or replaced.

Stu Summer   100 W

100 W
Posts: 100
Joined: Apr 27 2016 8:01pm
Location: Hillsdale, NY

Re: New 52v battery sat unused for two years...

Post by Stu Summer » Jul 16 2019 1:42pm

Thanks everyone for you cautions. I let it go!
2013 DB Haanjo Commuter with BBSHD and Zzipper fairing
Marin Rift Zone FS with BBSHD
Kysmo "lab" bike with 350w hub motor
Ryan Vanguard recumbent LWB with a 36v Cyclone 350w middrive and a 56v MAC 5t in the front hub.

Post Reply