Search found 1 match

by richie241
Jan 12 2020 1:16pm
Forum: Battery Technology
Topic: Li-ion cells cycle ageing
Replies: 441
Views: 46906

Re: Li-ion cells cycle ageing

It takes about 11 weeks to do 500 cycles. My intention is to finish testing at latest 700 cycles. I suppose for most of community will be 700 cycles data informative enough and testing another cells will be more interesting. Moreover, we havenĀ“t enough time frame for long term testing. It is your t...